Please wait a minute...
Acta Metall Sin  2009, Vol. 45 Issue (7): 866-872    DOI:
论文 Current Issue | Archive | Adv Search |
EFFECTS OF LOADING RATE, NOTCH GEOMETRY AND LOADING MODE ON THE CLEAVAGE FRACTURE BEHAVIOR OF 16MnR STEEL
WANG Guozhen1;  WANG Yuliang2;  XUAN Fuzhen1; TU Shantung1; WANG Zhengdong1
1) Key Laboratory of Safety Science of Pressurized System; Ministry of Education; School of Mechanical and Power Engineering; East China University of Science and Technology; Shanghai 200237
2) State Key Laboratory of Advanced Non--Ferrous Metal Materials; Lanzhou University of Technology; Lanzhou 730050
Cite this article: 

WANG Guozhen WANG Yuliang XUAN Fuzhen TU Shantung WANG Zhengdong. EFFECTS OF LOADING RATE, NOTCH GEOMETRY AND LOADING MODE ON THE CLEAVAGE FRACTURE BEHAVIOR OF 16MnR STEEL. Acta Metall Sin, 2009, 45(7): 866-872.

Download:  PDF(1256KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

The changes in loading rate and test temperature influence deformation (yield and flow) and fracture behavior of steel. The most significant effect of increasing loading rate is to shift the quasi--static fracture toughness transition curve toward higher temperatures, that is, to raise the temperatures at which cleavage may occur. This is very critical for structural steel components. The high strain rate sensitivity of these steels makes the safety design on the basis of quasi--static behavior rather poor. Therefore, the reliability of structures possibly loaded at higher loading rates requires the knowledge of the corresponding material fracture behavior. However, the effects of loading rate on the cleavage fracture mechanism, fracture stress and toughness of various steels have not been understood completely. Specifically, the prediction of the cleavage fracture behavior in notched specimens and actual structures and components loaded at various loading rates remain to be learned. In engineering structures and components possibly loaded at various loading rates, notch defects may be difficult to avoid and some notch--like geometries are necessary for structure design. Therefore, the understanding of notch toughness at various loading rates is also very important. In this work, the effects of loading rate, notch geometry and loading mode on the cleavage fracture behavior of 16MnR steel were studied by experiments and FEM calculations. The results show that the cleavage fracture mechanism of this steel, the corresponding local cleavage fracture stress σf and macroscopic cleavage fracture stress σF do not change with the above three factors. The change of the notch toughness of the notched specimens with different notch geometries and loading modes with loading rates can be predicated by the criterion σyymax≧σF, where σyymax is the maximum normal stress ahead of a notch and can be obtained by FEM calculations. The σF can be regarded as an engineering notch toughness parameter, and may be used for assessing the integrity of structures with notch defects. The σF values of steels can be measured by the Griffiths--Owen notched specimen at prescribed test temperature and loading rate.

Key words:  16MnR steel      cleavage fracture      loading rate      notched specimen      stress      loading mode     
Received:  10 December 2008     
ZTFLH: 

TG111.91

 
Fund: 

Supported by National High Technology Research and Development Program of China (Nos.2008AA04Z347 and 2006AA04Z413) and National Natural Science Foundation of China (No.50835003)

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2009/V45/I7/866

[1] Couque H, Asaro R J, Duffy J, Lee S H. Metall Trans, 1988; 19A: 2179
[2] Zurek A K, Follansbee P S, Hack J. Metall Trans, 1990; 21A: 431
[3] Lee S, Rhyu J W, Cho K M, Duffy J. Metall Trans, 1993; 24A: 901
[4] Venkert A, Guduru P R, Ravichandran G. Metall Mater Trans, 2000; 31A: 1147
[5] Wang G Z, Ren X C, Chen J H. Metall Mater Trans, 2004; 35A: 1765
[6] Wang G Z, Liu Y G, Chen J H. Mater Sci Eng, 2004; A369: 181
[7] Mendiratta M G, Goetz R L, Dimiduk D M. Metall Mater Trans, 1996; 27A: 3903
[8] Wang G Z, Chen J H. Int J Fract, 1998; 89: 269
[9] Chen J H, Wang G Z, Yan C, Ma H, Zhu L. Int J Fract, 1997; 83: 105
[10] Wang G Z, Wang H J, Chen J H. Fatigue Fract Eng Mater Struct, 1999; 22: 849
[11] Chen J H, Zhu L, Ma H. Acta Metall Mater, 1990; 38: 2527
[12] Griffiths J R, Owen D R J. J Mech Phys Solids, 1971; 19: 419

[1] DU Jinhui, BI Zhongnan, QU Jinglong. Recent Development of Triple Melt GH4169 Alloy[J]. 金属学报, 2023, 59(9): 1159-1172.
[2] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[3] LI Shilei, LI Yang, WANG Youkang, WANG Shengjie, HE Lunhua, SUN Guang'ai, XIAO Tiqiao, WANG Yandong. Multiscale Residual Stress Evaluation of Engineering Materials/Components Based on Neutron and Synchrotron Radiation Technology[J]. 金属学报, 2023, 59(8): 1001-1014.
[4] LI Qian, LIU Kai, ZHAO Tianliang. Rust Formation Behavior and Mechanism of Q235 Carbon Steel in 5%NaCl Salt Spray Under Elastic Tensile Stress[J]. 金属学报, 2023, 59(6): 829-840.
[5] LIANG Kai, YAO Zhihao, XIE Xishan, YAO Kaijun, DONG Jianxin. Correlation Between Microstructure and Properties of New Heat-Resistant Alloy SP2215[J]. 金属学报, 2023, 59(6): 797-811.
[6] HAN En-Hou, WANG Jianqiu. Effect of Surface State on Corrosion and Stress Corrosion for Nuclear Materials[J]. 金属学报, 2023, 59(4): 513-522.
[7] CHANG Litao. Corrosion and Stress Corrosion Crack Initiation in the Machined Surfaces of Austenitic Stainless Steels in Pressurized Water Reactor Primary Water: Research Progress and Perspective[J]. 金属学报, 2023, 59(2): 191-204.
[8] ZHANG Zixuan, YU Jinjiang, LIU Jinlai. Anisotropy of Stress Rupture Property of Ni Base Single Crystal Superalloy DD432[J]. 金属学报, 2023, 59(12): 1559-1567.
[9] WANG Chongyang, HAN Shiwei, XIE Feng, HU Long, DENG Dean. Influence of Solid-State Phase Transformation and Softening Effect on Welding Residual Stress of Ultra-High Strength Steel[J]. 金属学报, 2023, 59(12): 1613-1623.
[10] ZHANG Kaiyuan, DONG Wenchao, ZHAO Dong, LI Shijian, LU Shanping. Effect of Solid-State Phase Transformation on Stress and Distortion for Fe-Co-Ni Ultra-High Strength Steel Components During Welding and Vacuum Gas Quenching Processes[J]. 金属学报, 2023, 59(12): 1633-1643.
[11] JIANG Jiang, HAO Shijie, JIANG Daqiang, GUO Fangmin, REN Yang, CUI Lishan. Quasi-Linear Superelasticity Deformation in an In Situ NiTi-Nb Composite[J]. 金属学报, 2023, 59(11): 1419-1427.
[12] QI Zhao, WANG Bin, ZHANG Peng, LIU Rui, ZHANG Zhenjun, ZHANG Zhefeng. Effects of Stress Ratio on the Fatigue Crack Growth Rate Under Steady State of Selective Laser Melted TC4 Alloy with Defects[J]. 金属学报, 2023, 59(10): 1411-1418.
[13] LU Haifei, LV Jiming, LUO Kaiyu, LU Jinzhong. Microstructure and Mechanical Properties of Ti6Al4V Alloy by Laser Integrated Additive Manufacturing with Alternately Thermal/Mechanical Effects[J]. 金属学报, 2023, 59(1): 125-135.
[14] MA Zhimin, DENG Yunlai, LIU Jia, LIU Shengdan, LIU Honglei. Effect of Quenching Rate on Stress Corrosion Cracking Susceptibility of 7136 Aluminum Alloy[J]. 金属学报, 2022, 58(9): 1118-1128.
[15] LI Xiaolin, LIU Linxi, LI Yating, YANG Jiawei, DENG Xiangtao, WANG Haifeng. Mechanical Properties and Creep Behavior of MX-Type Precipitates Strengthened Heat Resistant Martensite Steel[J]. 金属学报, 2022, 58(9): 1199-1207.
No Suggested Reading articles found!