| RESEARCH ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF A NEW WROUGHT SUPERALLOY |
| ;;; |
| 北京科技大学 |
|
Cite this article:
;. RESEARCH ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF A NEW WROUGHT SUPERALLOY. Acta Metall Sin, 2008, 44(5): 540-546 .
|
|
|
Abstract The microstructure of a new wrought superalloy under standard heat treatment condition was studied by means of thermodynamic calculation, optical microscope, scanning electron microscopy, transmission electron microscopy and chemical phase analysis. The main mechanical properties were given for comprehensively understanding
the tested alloy. The results indicate that the tested alloy under standard heat treatment condition is composed of equiaxed grains with different sizes. The spheric γ′(Ni3(Al,Ti)) is the main strengthening phase of the alloy and distribute dispersedly in the matrix whose size is very small.Cr23C6 and a few (Ti,Mo)C mainly precipitate on the grain boundaries and some of them precipitate in intracrystalline. Besides, There are very few M6C in the tested alloy. The tested alloy under standard heat treatment condition not only has higher strength but has better plasticity and ductility, has higher creep strength than that of Waspaloy alloy.
|
|
Received: 03 July 2007
|
|
|
[1]Hu Z Q,Peng P,Liu T,Jin T,Sun X F,Guan H R.Acta Metall Sin,2002;38:1121 (胡壮麒,彭平,刘铁,金涛,孙晓峰,管恒荣.金属学报,2002;38:1121) [2]Klarstrom D L,Ishwar V R,Rowe M D.Acta Metall Sin (Engl Lett),2005;18:5 [3]Mao J,Chang K-M,Yang W H,Furrer D U,Ray K,Vaze S P.Mater Sci Eng,2002;A332:318 [4]Pike L M.Haynes International Technical Report, No.91204,Kokomo,IN:Haynes International Inc.,2006 [5]Haynes International Inc.,USA.Haynes 282TM Alloy. No.H-3172,Kokomo,IN:Haynes International Inc.,2005 [6]Pike L M.Haynes International Technical Report No.28267,Kokomo,IN:Haynes International Inc.,2007 [7]Sundman B,Jansson B,Anderson J O.CALPHAD,1985; 9:153 [8]Schaifernak B C,Cerjak H H.CALPHAD,2001;25:241 [9]Zhao J C,Ravikumar B,Beltran A M.Metall Mater Trans,2001;32A:1271 [10]Penkalla H J,Wosik J,Czyrska-Filemonowicz A.Mater Chem Phys,2003;81:417 [11]Ma W Y,Han Y F,Li S S,Zheng Y R,Gong S K.Acta Metall Sin,2006;42:1191 (马文有,韩雅芳,李树索,郑运荣,宫声凯.金属学报,2006;42:1191) [12]Rowe M D.Weld J,2006;85(2):31 |