| STUDY ON MICROSTRUCTURE SIMULATION OF ZL114A ALLOY DURING LOW PRESSURE DIE CASTING PROCESS |
| Bin Li;;;Baicheng LIU;;; |
| 清华大学机械系 |
|
Cite this article:
Bin Li; Baicheng LIU. STUDY ON MICROSTRUCTURE SIMULATION OF ZL114A ALLOY DURING LOW PRESSURE DIE CASTING PROCESS. Acta Metall Sin, 2008, 44(2): 243-248 .
|
|
|
Abstract A nucleation model based on the statistical analysis of a number of experimental data was developed and the related thermodynamics and kinetics parameters were presented for low pressure die casting of ZL114A alloy. A modified CA-FD method was proposed to simulate macro solidification process and microstructure evolution of the alloy. The preferential growth orientation, the solute redistribution in both liquid and solid, the solid/liquid interface curvature and the growth anisotropy were all considered in the model. The grain size, secondary dendrite arm spacing and eutectic content volume fraction of the alloy at different cooling rate were predicted and compared with experimental results of step-shaped sample casting.
|
|
Received: 18 April 2007
|
[1]Li M E,Wang Y X,Yang G C,Xing J D.Mech Sci Tech- nol,2002;21:824 (李梅娥,王友序,杨根仓,邢建东.机械科学与技术,2002;21:824) [2]Chen L L,Liu R X,Lin H T,Pan Z Y,Zhi Q M,Wu Z Y.Spec Cast Nonferr Alloy,2002;(s1):173 (陈立亮,刘瑞祥,林汉同,潘增源,支前明,吴祖宴.特种铸造及有色合金,2002;(s1):173) [3]Cheng W L,Xiong S M,Liu B C.Foundry,2003;52:609 (程万里,熊守美,柳百成.铸造,2003;52:609) [4]Wan L J,Zhang H,Jing T.Hot Work Technol,2005;(12): 27 (万柳军,张辉,荆涛.热加工工艺,2005;(12):27) [5]Nastac L.Acta Mater,1999;47:4253 [6]Liu Y,Xu Q Y,Liu B C.Tsinghua Sci Technol,2006;11: 495 [7]Liang Z J,Xu Q Y,Li J R,Yuan H L,Liu S Z,Liu B C. Acta Metall Sin,2004;40:439 (梁作俭,许庆彦,李嘉荣,袁海龙,刘世忠,柳百成.金属学报,2004;40:439) [8]Zhu M F,Hong C P.Metall Mater Trans,2004;35A:1555 [9]Zhu M F,Chen J,Sun G X,Hong C P.Acta Metall Sin, 2005;41:583 (朱鸣芳,陈晋,孙国雄,洪俊杓.金属学报,2005;41:583) [10]Beltran-Sanchez L,Stefanescu D M.Metall Mater Trans, 2003;34A:367 [11]Li Q,Li D Z,Qian B N.Acta Metall Sin,2004;40:634 (李强,李殿中,钱百年.金属学报,2004;40:634) [12]Wang Q G,Davidson C J.J Mater Sci,2001;36:739 [13]Thěvoz Ph,Desbiolles J-L,Rappaz M.Metall Mater Trans,1989;20A:311 [14]Rappaz M,Boettinger W J.Acta Mater,1999;47:3205 [15]Thompson C V,Spaepen F.Acta Metall,1983;31:2021 [16]Zhang X Z.Acta Mater,1998;46:1135 [17]Cheng Z W.PhD Dissertation,Northwestern Polytechni- cal University,Xi'an,2003:57 (陈忠伟.西北工业大学博士学位论文,西安,2003:57) [18]Zhu M F,Kim J M,Hong C P.ISIJ Int,2001;41:992Y |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|