| Microstructure and Transformation Behavior of Ni-Ti-Nb Shape Memory Alloys with Low Nb Content |
| YANG Yazhuo; ZHAO Xinqing; MENG Lingjie; YANG Shanglin; XU Huibin |
| School of Materials Science and Engineering; Beijing University of Aeronautics and Astronautics; Beijing 100083;Electronic Engineering Department; Harbin Engineering University; Harbin 150001 |
|
Cite this article:
YANG Yazhuo; ZHAO Xinqing; MENG Lingjie; YANG Shanglin; XU Huibin. Microstructure and Transformation Behavior of Ni-Ti-Nb Shape Memory Alloys with Low Nb Content. Acta Metall Sin, 2005, 41(6): 627-632 .
|
|
|
Abstract The structure evolution and phase transformation behavior of Ni-Ti-Nb shape
memory alloys with 4.5%Nb (atomic fraction) were studied systematically. It is
found that the structure evolution as well as the phase transformation
characteristics of the alloys is very sensitive to the ratio of the atomic
fractions of Ni and Ti. After appropriate predeformation, a wide hysteresis
was observed in such low Nb alloys. The difference of the mechanical behaviors
of the alloys with austenite or martensite states was investigated at the
same temperature, and explained by the kinetics of thermoelastic martensitic
transformation.
|
|
Received: 18 September 2004
|
|
|
[1]Otsuka K,Wayman C M.Shape Memory Materials.Lon- don:Cambridge University Press,1998 [2]Otsuka K,Kakeshita T.MRS Bull,2002;27:91 [3]Duerig T W,Melton K,Proft J L.In:Duerig T W,ed., Engineering Aspects of Shape Memory Alloys.London: Butterworth-Heinemann Ltd.,1990:130 [4]Piao M,Miyazaki S,Otsuka K.Mater Trans JIM,1992;34:919 [5]Zhao X Q,Wang E M,Zhao W B,Zhao Z Y,Han Y F.J Aeron Mater,2000:20(2):8 (赵新清,王二敏,赵伟彪,赵振业,韩雅芳,航空材料学报,2000;20(2):8) [6]Yang J H,Simpson J W.J Phys Colloq,1995;5(C8):771 [7]Piao M,Miyazaki S,Otsuka K.Mater Trans JIM,1992;33:337 [8]Jin W.PhD Dissertation,Institute of Metal Research, The Chinese Academy of Sciences,Shenyang,2002 (金伟.中国科学院金属研究所博士学位论文,沈阳,2002) [9]Zhao L C,Duerig T W,Justi S,Melton K N,Proft J L, Yu W,Wayman C M.Scr Metall Mater,1990;24:221 [10]Zhang C S,Cai W,Wang Y Q,Zhao L C.Chin J Non-ferrous Met,1994;4:82 (张春生,蔡伟,王永前,赵连城.中国有色金属学报,1994;4:82) [11]Melton K N.In:Duerig T W,ed.,Engineering Aspects of Shape Memory Alloys.London:Butterworth-Heinemann Ltd.,1990:21 [12]Piao M,Miyazaki S,Otsuka K.Mater Trans JIM,1992; 33:346 [13]Tong H G,Wayman M.Acta Metall,1974;22:887 [14]Zhang C S,Zhao L C,Duerig T W,Wayman C M.Scr Metall Mater,1990;24:1807 [15]Zheng Y J,Cui L S,Zhang F.J Mater Sci Technol,2000; 16:611 [16]He X M,Rong L J,Yan D S,Li Y Y.Mater Sci Eng, 2004;A371:193 [17]He X M,Rong L J,Yan D S,Jiang Z M,Li Y Y.Acta Metall Sin,2004;40:721 (何向明,戎利建,闫德胜,姜志民,李依依.金属学报,2004;40:721)A |