| Oxidation Behaviors of Ti44Ni47Nb9 Shape Memory Alloy at High Temperature |
| TAO Binwu; LIU Jianhua; LI Songmei |
| School of Materials Science and Engineering; Beijing University of Aeronautics and Astronautics; Beijing 100083 |
|
Cite this article:
TAO Binwu; LIU Jianhua; LI Songmei. Oxidation Behaviors of Ti44Ni47Nb9 Shape Memory Alloy at High Temperature. Acta Metall Sin, 2005, 41(6): 633-637 .
|
|
|
Abstract The isothermal oxidation resistance of Ti44Ni47Nb9 shape
memory alloy (SMA) in air over the temperature range of 450-850 ℃ was
studied by using XRD, SEM and EDS techniques. Light oxidation was found
on the alloy surface at 450 ℃. The alloy was attacked by oxidation and
the oxidation kinetic curves were approximately parabola within the
temperature range of 600—800 ℃. Experimental results indicate that a
multi-layered scale was formed, consisting of an outer rutile layer, a
Nb rich intermediate layer and a thin inner Ni3Ti layer. It was found
that the Nb rich intermediate layer was compact, which obviously improved
the oxidation resistance of the alloy due to its effective inhibition to
diffusion of oxygen and titanium. Furthermore, the internal oxidation of
nickel element was also inhibited because of the existence of Nb rich
layer, which reduced oxygen concentration in the alloy.
|
|
Received: 14 September 2004
|
|
|
[1]Kajiwara S.Mater Sci Eng,1999;A273-275:67 [2]Piao M,Miyazakai S,Otsuka K.Mater Trans JIM,1992; 33:337 [3]Cai W,Zhang C C.J Mater Sci Technol,1994;10:27 [4]Yang H B,Yin W H,Lin J Y,Zhang X M,Guo J H.Rare Met Mater Eng,1999;28:81 (杨华斌,殷为宏,吝靖玉,张小明,郭继红.稀有金属材料与工程,1999;28:81) [5]Dong Z Z,Liu W X,Jia D,Tang Z L,Wang D F.Rare Met Mater Eng,2000;29:182 (董治中,刘文西,贾堤,唐子龙,王德法.稀有金属材料与工程,2000;29:182) [6]Mo H Q,Li C,Wang C L,Qiu S Y,Huang D C,Shen B L.Nucl Power Eng,2003;24:559 (莫华强,李聪,王丛林,邱绍宇,黄德成,沈保罗.核动力工程,2003;24:559) [7]Long N D,Zhu J H.Rare Met Mater Eng,2003;32:740 (龙霓东,朱金华.稀有金属材料与工程,2003;32:740) [8]He X M,Rong L J,Yan D S,Jiang Z M,Li Y Y.Ada Metall Sin,2004;40:721 (何向明,戎利建,阎德胜,姜志民,李依依.金属学报,2004;40:721) [9]Xu C H,Ma X Q,Shi S Q,Wo C H.Mater Sci Eng,2004;A371:45 [10]Liu Y H.Theory of Metal Corrosion.Beijing:Aeronautics Industry Press,1993:186 (刘永辉.金属腐蚀原理.北京:航空工业出版社,1993:186) [11]Gesmundo F,Niu Y,Viani F.Oxid Met,1996;46:441 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|