Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (5): 489-496    DOI:
Current Issue | Archive | Adv Search |
RAPID SOLIDIFICATION OF UNDERCOOLED Co_(85)Cu_(15) HYPOPERITECTIC ALLOY
CAO Chongde; LU Xiaoyu; WEI Bingbo (Department of Applied Physics; Northwestern Polytechnical University; Xi'an 710072)
Cite this article: 

CAO Chongde; LU Xiaoyu; WEI Bingbo (Department of Applied Physics; Northwestern Polytechnical University; Xi'an 710072). RAPID SOLIDIFICATION OF UNDERCOOLED Co_(85)Cu_(15) HYPOPERITECTIC ALLOY. Acta Metall Sin, 1998, 34(5): 489-496.

Download:  PDF(1925KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Co85Cu15 hypoperitectic alloy melt was undercooled by 351 K (0.21TL ) with glass fluxing technique. The hypercooling limit of this alloy was determined to be 379 K. With increasing undercooling temperature, the microstructure transformed from dendrites into equiaxed grains and was refined drastically. Significant solute trapping has taken place during the rapid solidification of highly undercooled Co85Cu15 alloy, and it resulted in the remarkable extension of solubility of Cu in Co phase and much weaker intragranular segregation. It was also revealed by X-ray diffraction that the microstructures were comprised mainly by metastable supersaturated α-Co and Cu solid solutions together with a small amount of ε-Co phase. In addition,the theoretical calculation for nucleation rate indicates that heterogeneous nucleation has still taken place at an undercooling of 351 K. Calculations of dendrite growth velocity, solubility of Cu in α-Co, partial undercoolings, and dendrite tip radius were also performed on the basis of LKT/BCT theory.
Key words:  peritectic alloy      liquid metal      undercooling      rapid solidification     
Received:  18 May 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I5/489

1 Wei B,Herlach D M.Sommer F,Kurz W.Mater Sci Eng,1994:A181/182 1150
2 Wu Y,Piccone T J,Shiohara Y,Flemings M C.Metall Trans;1987:18A:915
3Jansen R,Sahm P R. Mater Sci Eng,1984:65:199
4Wei B, Herlach D M, Feuerbacher B, Sommer F. Acta Metall Mater, 1993: 41: 1801
5Tewari S N Metall Trans; 1987; 18A: 525
6Alien W P, Perepezko J H Metall Trans, 1991: 22A: 753
7Elder S P, Munitz A, Abbaschian G J Mater Sci Forum, 1989: 50: 137
8Munitz A, Elder-Randall S P, Abbaschian R. Metall Truns A,1992: 23: 1817
9Munitz A, Abbaschian R. J Mater Sci, 1991; 26: 6458
10魏炳波,董长星.金属学报,1996;32:357(Wei Bingbo,Dong Changxing Acta Metall Sin.1996;32:357)
11Lipton J, Kurz W; Trivedi R. Acta Metall, 1987; 35: 967
12Trivedi R, Lipton J, Kurz W Acta Metall, 1987; 35: 965
13Boettinger W J,Coriell A R,Trivedi R In:Mehrabian R.Parrish P A eds,Proc 4th Conf on Rapid Solidification Processing:Principles and Technologies Baton Rouge:Claitors,1987:13
14Wei B, Herlach D M. Mater Sci Eng、 1993 173A: 357#
[1] WU Xinqiang, RONG Lijian, TAN Jibo, CHEN Shenghu, HU Xiaofeng, ZHANG Yangpeng, ZHANG Ziyu. Research Advance on Liquid Lead-Bismuth Eutectic Corrosion Resistant Si Enhanced Ferritic/Martensitic and Austenitic Stainless Steels[J]. 金属学报, 2023, 59(4): 502-512.
[2] LIANG Chen, WANG Xiaojuan, WANG Haipeng. Formation Mechanism of B2 Phase and Micro-Mechanical Property of Rapidly Solidified Ti-Al-Nb Alloy[J]. 金属学报, 2022, 58(9): 1169-1178.
[3] XU Junfeng, ZHANG Baodong, Peter K Galenko. Model of Eutectic Transformation Involving Intermetallic Compound[J]. 金属学报, 2021, 57(10): 1320-1332.
[4] Kuanhui HU, Xinping MAO, Guifeng ZHOU, Jing LIU, Zhifen WANG. Effect of Si and Mn Contents on the Microstructure and Mechanical Properties of Ultra-High Strength Press Hardening Steel[J]. 金属学报, 2018, 54(8): 1105-1112.
[5] Yun LI, Lianjie LIU, Xinming LI, Jinfu LI. Solidification of Undercooled Co75B25 Alloy[J]. 金属学报, 2018, 54(8): 1165-1170.
[6] Dandan FAN, Junfeng XU, Yanan ZHONG, Zengyun JIAN. Effect of Superheated Temperature and Cooling Rate on the Solidification of Undercooled Ti Melt[J]. 金属学报, 2018, 54(6): 844-850.
[7] Zengyun JIAN, Tao XU, Junfeng XU, Man ZHU, Fang'e CHANG. Development of Solid-Liquid Interfacial Energyof Melt-Crystal[J]. 金属学报, 2018, 54(5): 766-772.
[8] Bin ZHAI, Kai ZHOU, Peng Lü, Haipeng WANG. Rapid Solidification of Ti-6Al-4V Alloy Micro-Droplets Under Free Fall Condition[J]. 金属学报, 2018, 54(5): 824-830.
[9] Lin LIU, Dejian SUN, Taiwen HUANG, Yanbin ZHANG, Yafeng LI, Jun ZHANG, Hengzhi FU. Directional Solidification Under High Thermal Gradient and Its Application in Superalloys Processing[J]. 金属学报, 2018, 54(5): 615-626.
[10] Guohua WU, Yushi CHEN, Wenjiang DING. Current Research and Future Prospect on Microstructures Controlling of High Performance Magnesium Alloys During Solidification[J]. 金属学报, 2018, 54(5): 637-646.
[11] Jinfu LI, Yaohe ZHOU. Remelting of Primary Solid in Rapid Solidification of Deeply Undercooled Alloy Melts[J]. 金属学报, 2018, 54(5): 627-636.
[12] Jianglei ZHU, Qing WANG, Haipeng WANG. Thermophysical Properties and Atomic Distribution of Undercooled Liquid Cu[J]. 金属学报, 2017, 53(8): 1018-1024.
[13] Qianqian GU, Ying RUAN, Haizhe ZHU, Na YAN. Influence of Cooling Rate on Microstructural Formation of Melt-Spun Fe-Al-Nb Ternary Alloy[J]. 金属学报, 2017, 53(6): 641-647.
[14] Xu YANG, Bo LIAO, Jian LIU, Wei YAN, Yiyin SHAN, Furen XIAO, Ke YANG. Embrittlement Phenomenon of China Low Activation Martensitic Steel in Liquid Pb-Bi[J]. 金属学报, 2017, 53(5): 513-523.
[15] Huogen HUANG,Hongyang XU,Pengguo ZHANG,Yingmin WANG,Haibo KE,Pei ZHANG,Tianwei LIU. U-Cr Binary Alloys with Anomalous Glass-Forming Ability[J]. 金属学报, 2017, 53(2): 233-238.
No Suggested Reading articles found!