CORROSION BEHAVIOR OF A STEEL 1Cr_(11)Ni_2W_2MoV COATED WITH NaCl IN WATER VAPOR AT 500-700℃
SHU Yonghua; WANG Fuhui; ZHOU Longjiang; WU Weitao (State Key Laboratory for Corrosion and Protection; Institute of Corrosion and Protection of Metals; The Chinese Academy of Sciences; Shenyang 110015)
Cite this article: 

SHU Yonghua; WANG Fuhui; ZHOU Longjiang; WU Weitao (State Key Laboratory for Corrosion and Protection; Institute of Corrosion and Protection of Metals; The Chinese Academy of Sciences; Shenyang 110015). CORROSION BEHAVIOR OF A STEEL 1Cr_(11)Ni_2W_2MoV COATED WITH NaCl IN WATER VAPOR AT 500-700℃. Acta Metall Sin, 1998, 34(5): 483-488.

Download:  PDF(2535KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The corrosion behavior of a steel 1Cr11Ni2W2MoV has been studied in the presence of NaCl and water vapor at 500 - 700 ℃. The results indicate that corrosion of the steel 1Cr11Ni2W2MoV was not obvious in the atmospheres without NaCl, while corrosion was severely speeded up when the atmosphere contained NaCl and water vapor. Optical microscope (OM),X-ray diffraction (XRD), scanning electron microscope (SEM) and electron probe microanalysis (EPMA) were used to analyse the corrosion products. The mechanism of the effect of water vapor and NaCl on corrosion of this steel was proposed.
Key words:  steel 1Cr_(11)Ni_2W_2MoV      NaCl and water vapor      corrosion     
Received:  18 May 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I5/483

1 Misra R D K, Sivakumar R. Oxid Met, 1986: 25: 83
2 Evans H E, Hilton D A, Holm R A, Simpson P W G Oxid Met、 1981: 16: 327
3 Bourhis Y, St John C Oxid Met, 1975 9: 507
4 Shinata Y,Takahashi F,Hashiura K Mater Sci Eng,1987: 87:399
5 Yao Z, Marek M Mater Sci Eng, 1995; 192: 994
6 张允书,李连方,石声泰.中国腐蚀与防护学报,1990; 10:275(Zhang Yunshu,Li Lianfang,Shi Shengtai.J Chin Soc Corros Prot.1990;10;275)
7 谢俊泉,宋士晖.北京科技大学学报,19962 18:518(Xie Junquan,Song Shihui .J Uni Sci Technol Beijing,1996 18:518)
8 Shen J N, Zhou L J, Li T F Oxid Met、 1997; 48: 347
9 董俊华.中国科学院金属腐蚀与防护研究所博士学位论文,1995(Dong Junhua PhD Dissertation ,Inshtute Corrsion Protection of Metals.The Chinese Academy of Scienses, 1995)
10 Shinata Y, Nishi Y. Oxid Met, 1986 26: 201
[1] LI Xiaohan, CAO Gongwang, GUO Mingxiao, PENG Yunchao, MA Kaijun, WANG Zhenyao. Initial Corrosion Behavior of Carbon Steel Q235, Pipeline Steel L415, and Pressure Vessel Steel 16MnNi Under High Humidity and High Irradiation Coastal-Industrial Atmosphere in Zhanjiang[J]. 金属学报, 2023, 59(7): 884-892.
[2] WANG Zongpu, WANG Weiguo, Rohrer Gregory S, CHEN Song, HONG Lihua, LIN Yan, FENG Xiaozheng, REN Shuai, ZHOU Bangxin. {111}/{111} Near Singular Boundaries in an Al-Zn-Mg-Cu Alloy Recrystallized After Rolling at Different Temperatures[J]. 金属学报, 2023, 59(7): 947-960.
[3] CHEN Runnong, LI Zhaodong, CAO Yanguang, ZHANG Qifu, LI Xiaogang. Initial Corrosion Behavior and Local Corrosion Origin of 9%Cr Alloy Steel in Cl-Containing Environment[J]. 金属学报, 2023, 59(7): 926-938.
[4] ZHANG Qiliang, WANG Yuchao, LI Guangda, LI Xianjun, HUANG Yi, XU Yunze. Erosion-Corrosion Performance of EH36 Steel Under Sand Impacts of Different Particle Sizes[J]. 金属学报, 2023, 59(7): 893-904.
[5] SI Yongli, XUE Jintao, WANG Xingfu, LIANG Juhua, SHI Zimu, HAN Fusheng. Effect of Cr Addition on the Corrosion Behavior of Twinning-Induced Plasticity Steel[J]. 金属学报, 2023, 59(7): 905-914.
[6] ZHAO Pingping, SONG Yingwei, DONG Kaihui, HAN En-Hou. Synergistic Effect Mechanism of Different Ions on the Electrochemical Corrosion Behavior of TC4 Titanium Alloy[J]. 金属学报, 2023, 59(7): 939-946.
[7] WANG Jingyang, SUN Luchao, LUO Yixiu, TIAN Zhilin, REN Xiaomin, ZHANG Jie. Rare Earth Silicate Environmental Barrier Coating Material: High-Entropy Design and Resistance to CMAS Corrosion[J]. 金属学报, 2023, 59(4): 523-536.
[8] HAN En-Hou, WANG Jianqiu. Effect of Surface State on Corrosion and Stress Corrosion for Nuclear Materials[J]. 金属学报, 2023, 59(4): 513-522.
[9] WU Xinqiang, RONG Lijian, TAN Jibo, CHEN Shenghu, HU Xiaofeng, ZHANG Yangpeng, ZHANG Ziyu. Research Advance on Liquid Lead-Bismuth Eutectic Corrosion Resistant Si Enhanced Ferritic/Martensitic and Austenitic Stainless Steels[J]. 金属学报, 2023, 59(4): 502-512.
[10] XU Linjie, LIU Hui, REN Ling, YANG Ke. Effect of Cu on In-Stent Restenosis and Corrosion Resistance of Ni-Ti Alloy[J]. 金属学报, 2023, 59(4): 577-584.
[11] LIAO Jingjing, ZHANG Wei, ZHANG Junsong, WU Jun, YANG Zhongbo, PENG Qian, QIU Shaoyu. Periodic Densification-Transition Behavior of Zr-Sn-Nb-Fe-V Alloys During Uniform Corrosion in Superheated Steam[J]. 金属学报, 2023, 59(2): 289-296.
[12] XIA Dahai, JI Yuanyuan, MAO Yingchang, DENG Chengman, ZHU Yu, HU Wenbin. Localized Corrosion Mechanism of 2024 Aluminum Alloy in a Simulated Dynamic Seawater/Air Interface[J]. 金属学报, 2023, 59(2): 297-308.
[13] CHANG Litao. Corrosion and Stress Corrosion Crack Initiation in the Machined Surfaces of Austenitic Stainless Steels in Pressurized Water Reactor Primary Water: Research Progress and Perspective[J]. 金属学报, 2023, 59(2): 191-204.
[14] HU Wenbin, ZHANG Xiaowen, SONG Longfei, LIAO Bokai, WAN Shan, KANG Lei, GUO Xingpeng. Corrosion Behavior of AlCoCrFeNi2.1 Eutectic High-Entropy Alloy in Sulfuric Acid Solution[J]. 金属学报, 2023, 59(12): 1644-1654.
[15] SONG Jialiang, JIANG Zixue, YI Pan, CHEN Junhang, LI Zhaoliang, LUO Hong, DONG Chaofang, XIAO Kui. Corrosion Behavior and Product Evolution of Steel for High-Speed Railway Bogie G390NH in Simulated Marine and Industrial Atmospheric Environment[J]. 金属学报, 2023, 59(11): 1487-1498.
No Suggested Reading articles found!