Abstract The microstructures and textures during recrystallization process in the aluminium sheet which had been longitudinally and transversely rolled were investigated. The oriented growth during the recrystallization was directly observed by transmission electron microscope and the orientation relationships of new grains were determined by electron diffraction. The pole figures were measured with X-ray diffraction goniometer and ODF's were calculated by Bunge's method. The results showed that recrystallized grains with some oriented relationship to the deformation matrix grew more rapidly than others, which leads to the final texture. In fcc metal, this orientation relationship is about 40° <111>.
|
|
Received: 18 September 1997
|
1Duggan B J,Sindel M、Kohlhoff G d,Lucke K.Acta Metall Mater,1990:38:103 2Liu Y L.Hu H,Hansen N Acta Metall Mater,1995;43:2395 3Andrade U,Meyers M A、Vecchio K S、Chokshi A H Acta Meter,1994;42:3183 4Kamijo T,Kataoka S,Inagaki H.Acta Metall Mater,1993:41:1713 5Hirsch J, Nes E,Lucke K Acta Metall Mater、1987 35:427 6Beck P A,Hu H Recrystallisation,Grain Growth and Textures,Metal Park,Ohio:American Society for Metals,1965:393 7毛卫民中国科学、1991;A3:311 8Bunge H J Texture Analysis in Materials Science London:Butterworths,1982:1M |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|