SPONTANEOUS MAGNETIZATION OF FERROMAGNET
WANG Yongzhong;ZHANG Zhidong;ZENG Dechang;YANG Zongquan;TANG Hong;QIAO Guiwen (Institute of Metal Research; Chinese Academy of Sciences;Shenyang 110015)
Cite this article: 

WANG Yongzhong;ZHANG Zhidong;ZENG Dechang;YANG Zongquan;TANG Hong;QIAO Guiwen (Institute of Metal Research; Chinese Academy of Sciences;Shenyang 110015). SPONTANEOUS MAGNETIZATION OF FERROMAGNET. Acta Metall Sin, 1997, 33(9): 981-986.

Download:  PDF(432KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  By introducing disordering energy Ed, an effective molecular field coefficient λ(T)as a function of thermal energy, the exchange interaction energy and disordering energy is proposed to intefpret spontaneous magnetization of ferromagnetic materials. Usingλ(T),the relationships betweem Tc, θp, and Ed / k and the relationships of (ρ/X)-T and (Ms,/M0)-(T/Tc)were derived. The results show that the curves of (ρ/X)-T and (Ms /M0)-(T/Tc)fit the experimental curves of Ni very well.
Key words:  spontaneous magnetization      exchange energy      disorder energy     
Received:  18 September 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I9/981

1Weiss P J Phys Redium.1907;6:661
2Heisenberg W Z Physik,1928;49:619
3Stoner E D.Proc Roy Soc,1936;A154:656
4Blschof R Kaldis E,Wachter P J Magn Magn Mater 1983;31-34:255
5Ogawa S.J Magn Magn Mater,1983;31-34:269
6Yomo S.J Magn Magn Mater,1983;31-34:331
7Hettiarachchi N F,Greenough R D,Fort D,Jones D W J Magn Magn Mater,1982;25:310
8Greenough R D,Hettiarachchi N F,Jones D W,Hubert J K J Magn Magn Mater,1982;29:67
9Mazumdar P,Bhagat S M.J Magn Magn Mater,1987;66:263
10Zach R Guillot M,Fruchart R.J Magn Magn Matel,1990;89:221
11Mattis D C.The Theory of Magnetism II.Berlin:Springer Verlag,1985:47
12Vonsouskii S V.Magnetism New York:Halsted Press,1974:500
13Oquchi T Prog Theor Phys,1955;13:148
14戴道生,钱昆明著.铁磁学(上册).北京:科学出版社,1987:386
15Kittel C.Introduction to Solid State Physics.New York:John Wiley Sons &Sons Inc,1976:461
16Weiss P,Forrer R Ann Phys,19265:153#
No related articles found!
No Suggested Reading articles found!