Please wait a minute...
Acta Metall Sin  1997, Vol. 33 Issue (3): 304-308    DOI:
Current Issue | Archive | Adv Search |
INTERGRANULAR CORROSION BEHAVIOUR OF IMPLANT STAINLESS STEEL DURING CORROSION FATIGUE
XIE Jianhui;WU Yinshun; ZHU Rizhang (Universily of Science and Technology Beijing;Beijing 100083)
Cite this article: 

XIE Jianhui;WU Yinshun; ZHU Rizhang (Universily of Science and Technology Beijing;Beijing 100083). INTERGRANULAR CORROSION BEHAVIOUR OF IMPLANT STAINLESS STEEL DURING CORROSION FATIGUE. Acta Metall Sin, 1997, 33(3): 304-308.

Download:  PDF(2902KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The behaviours of intergranular corrosion on the rolled 316L and cast 317L implant stainless steels were studied by using SEM in the process of corrosion fatigue in Hank physiological solution. It was concluded that the initial fatigue cracks engender at the corroded granular boundaries and propagate along intergranule first and then transgranule under the fatigue stress. The intergranular corrosion is not due to the chrome-deficiency induced by the precipitation of carbide at the granular boundary but due to non-sensitized intergranular corrosion.
Key words:  intergranular corrosion      implant stainless steel      corrosion fatigue      Hank physiological solution     
Received:  18 March 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I3/304

1浦素云.金属植入材料及其腐蚀北京:北京航空航天大学出版社,1990:72
2 Cahoon J R.J Biomed Mater Res,1981;15:137
3 Buchanan R A,Ringey E D Jr,Williams J M.J Biomed Mater Res,1987;121:355
4谢建辉,吴荫顺,朱日彰全国第二届青年学术会卫星会议一第四届青年腐蚀与防护学术研讨会论文集,泰安,1995:187
[1] WANG Zongpu, WANG Weiguo, Rohrer Gregory S, CHEN Song, HONG Lihua, LIN Yan, FENG Xiaozheng, REN Shuai, ZHOU Bangxin. {111}/{111} Near Singular Boundaries in an Al-Zn-Mg-Cu Alloy Recrystallized After Rolling at Different Temperatures[J]. 金属学报, 2023, 59(7): 947-960.
[2] ZHENG Chun, LIU Jiabin, JIANG Laizhu, YANG Cheng, JIANG Meixue. Effect of Tensile Deformation on Microstructure and Corrosion Resistance of High Nitrogen Austenitic Stainless Steels[J]. 金属学报, 2022, 58(2): 193-205.
[3] TAN Jibo, WANG Xiang, WU Xinqiang, HAN En-Hou. Corrosion Fatigue Behavior of 316LN Stainless Steel Hollow Specimen in High-Temperature Pressurized Water[J]. 金属学报, 2021, 57(3): 309-316.
[4] Chao CAI,Yang LI,Jinfeng LI,Zhao ZHANG,Jianqing ZHANG. Correlation Between Ageing Precipitation, Potential and Intergranular Corrosion of 2A97 Al-Li Alloy Sheet[J]. 金属学报, 2019, 55(8): 958-966.
[5] Shenghu CHEN, Lijian RONG. Microstructure Evolution During Solution Treatment and Its Effects on the Properties of Ni-Fe-Cr Alloy[J]. 金属学报, 2018, 54(3): 385-392.
[6] Xiaosong ZHANG,Yong XU,Shihong ZHANG,Ming CHENG,Yonghao ZHAO,Qiaosheng TANG,Yuexia DING. Research on the Collaborative Effect of Plastic Deformation and Solution Treatment in the Intergranular Corrosion Property of Austenite Stainless Steel[J]. 金属学报, 2017, 53(3): 335-344.
[7] Xianfeng ZHANG,Guoai LI,Zheng LU,Juan YU,Min HAO. EFFECT OF PREAGED STRETCH AFTER QUENCHED ON THE PROPERTIES AND MICROSTRUCTURE OF A NATURALLY AGED Al-Li ALLOY[J]. 金属学报, 2016, 52(12): 1497-1502.
[8] YANG Hui, XIA Shuang, ZHANG Zilong, ZHAO Qing, LIU Tingguang, ZHOU Bangxin, BAI Qin. IMPROVING THE INTERGRANULAR CORROSION RESISTANCE OF THE WELD HEAT-AFFECTED ZONE BY GRAIN BOUNDARY ENGINEERING IN 304 AUSTENITIC STAINLESS STEEL[J]. 金属学报, 2015, 51(3): 333-340.
[9] WU Xinqiang, TAN Jibo, XU Song, HAN En-Hou, KE Wei. CORROSION FATIGUE MECHANISM OF NUCLEAR-GRADE LOW ALLOY STEEL IN HIGH TEMPERATURE PRESSURIZED WATER AND ITS ENVIRONMENTAL FATIGUE DESIGN MODEL[J]. 金属学报, 2015, 51(3): 298-306.
[10] Shaoming QIANG,Laizhu JIANG,Jin LI,Tianwei LIU,Yanping WU,Yiming JIANG. EVALUATION OF INTERGRANULAR CORROSION SUSCEPTIBILITY OF 11Cr FERRITIC STAINLESS STEEL BY DL-EPR METHOD[J]. 金属学报, 2015, 51(11): 1349-1355.
[11] LI Hai, MAO Qingzhong, WANG Zhixiu, MIAO Fenfen, FANG Bijun, SONG Renguo, ZHENG Ziqiao. EFFECT OF HIGH TEMPERATURE PRE-AGEING AND LOW-TEMPERATURE RE-AGEING ON MECHANICAL PROPERTIES AND INTERGRANULAR CORROSION SUSCEPTIBILITY OF Al-Mg-Si-Cu ALLOYS[J]. 金属学报, 2014, 50(11): 1357-1366.
[12] LI Xiangliang, CHEN Jianghua, LIU Chunhui, FENG Jiani, WANG Shihao. EFFECTS OF T6 AND T78 TEMPERS ON THE MICROSTRUCTURES AND PROPERTIES OF Al-Mg-Si-Cu ALLOYS[J]. 金属学报, 2013, 49(2): 243-250.
[13] GUO Lifang LI Xuyan SUN Tao XU Juliang LI Jin JIANG Yiming . THE INFLUENCE OF SENSITIVE TEMPERATURE ON THE LOCALIZED CORROSION RESISTANCE OF DUPLEX STAINLESS STEEL SAF2304[J]. 金属学报, 2012, 48(12): 1503-1509.
[14] WU Xinqiang XU Song HAN En-Hou KE Wei. CORROSION FATIGUE OF NUCLEAR--GRADE STAINLESS STEEL IN
HIGH TEMPERATURE WATER AND ITS ENVIRONMENTAL FATIGUE DESIGN MODEL
[J]. 金属学报, 2011, 47(7): 790-796.
[15] HAN En--Hou. RESEARCH TRENDS ON MICRO AND NANO--SCALE MATERIALS DEGRADATION IN NUCLEAR POWER PLANT[J]. 金属学报, 2011, 47(7): 769-776.
No Suggested Reading articles found!