MATERIALS DESIGN AGAINST FRACTURE |
XIAO Jimei (HSIAO Chimei) (University of Science and Technology Beijing; Beiing 100083) |
|
Cite this article:
XIAO Jimei (HSIAO Chimei) (University of Science and Technology Beijing; Beiing 100083). MATERIALS DESIGN AGAINST FRACTURE. Acta Metall Sin, 1997, 33(2): 113-125.
|
Abstract From methodological point of view, the concepts of failure, property and structure are clarified, their relationship and methods of analyses discussed. The design of materials against the following three types of fracture are elucidated: (1) Creep ruptureSystematic development of new alloy systems, establishment of phenomenalogical equations about property, structure and their relationship for design purpose; (2) Intergranular fracture-Phenomenalogical equation between the grain boundary concentration of impurity and the solid solubility of the impurity is obtained by induction method; the effect of grain boundary impurity on the work of intergranular fracture is derived with quasichemical theory; and the expert system is established; (3) Environmental cracking-The results of mechanism research are used to set up the guide lines for improvement and design of materials.
|
Received: 18 February 1997
|
1肖纪美,朱逢吾. 新材料研究,第二届中国材料研讨会论文集,北京:中国科协学会工作部,1988:1 2肖纪美. 材料学的方法论. 北京:冶金上业出版社,1994: 185 3盐见弘著.杨家铿等译.失效物理基础.北京:科学出版社,1982 4Kaelble D H.Computer-Aided Design of Polymers. New York: Marcel Dekker,1985 5肖纪美.大自然探索,1987; 3(2):5 6肖纪美.金属的韧性与韧化上海:上海科学技术出版社, 1980:17 7肖纪美机械强度,1995;17(2): 61 8Xiao Jimei. Modeling and Simulation in Metallurgical Engineering and Materials Science,Beijing:Metallurgical Industry Press, 1996:721 9Eberhardt J J. Hay P J, Carpenter Jr JA. Computor—based Microscopic Description of the Structure of Materials,Mat Res Soc Symp Proc,1986;89: 191 10 汤川厦夫. d电子合金设计及关连论文集,日本丰桥技术科学大学,1986 11 Pettifer DG.In:Cahn RW,Haasen P ed., Physical Metallurgy, Amsterdam: North Holland Physics Pub,1983:73 12 Savitsky E M,Gribuya V B.Application of Computer Techniques in Prediction of Inorganic Compounds, English Translation, New Delhi:Xonian Press,1985 13陈念贻.科学通报,1976;(5)216 14肖纪美.不锈钢的金属学问题北京:冶金工业出版社,1983:90 15肖纪美.金属学报, 1958; 3:138 16 Murrell J N,Kettle S F,Tedder J M.Chemical Bond.New York:John Wiley, 198517 Decker R F.Melall TranS,1973 3:2495 18 Kasak A Hsiao C. Dulis E J Proc ASTM,1959 59:786 19 Hondros E D,Seah M P,In:Cahn R W,Hassen P eds,Physical Metallurgy, Amsterdam:North Holland Physics, 1983:855 20 张瑷,余冬玲,梁成广,朱逢各,肖纪美.中国科学,1992; 22A:665 21 Seah M P.Acta Metall, 1980; 28:955 22 梁成广,张跷余冬玲,朱逢吾,肖纪美.中国科学,1993;23A:211 23 Pauling L.The Nature of Chemical Bond, 3rd ed.Ithaca:Comell Univ.Press,1961 24 Hsiao C, Chu W Y.Hydrogen Effects in Metals, Moran, Wyoming: Metall Soc of AIME, 1980: 255 25 Hsiao C.Mechanical Behavior of Materials-V, Pergamon Press, 1987:141 26 Hsiao C.Hydrogen and Materials. Beijing: Tsinghua Univ.,1988:502 27 Hsiao C.Hydrogen Effects on Materials Behavior, Moran, Wyoming: Metals, Material Soc, 1989:845 28 Hsiao C.Corrosion Control, 7th APCCC.1991:1 29 Hsiao C,Chu W.Zhu F Hydrogen Effects on Materials Behavior,Mineras,Metals,Materials Soc,1996:555 30 Xiao J. Failure Analysis and Prevention 1995,Beijing: Inte-Academic Pub, 1995:25 31肖纪美. 材料科学进展.北京:科学出版社,1986:13 32肖纪美.应力作用下的金属腐蚀北京:化学工业出版社,1990a |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|