| FORMATION MECHANISM OF NiAl/TiC NANOCOMPOSITE BY MECHANICAL ALLOYING |
| ZHOU Lanzhang;GUO Jianting;QUAN Mingxiu(Institute of Metal Research;The Chinese Academy of Sciences;Shenyang 110015) |
|
Cite this article:
ZHOU Lanzhang;GUO Jianting;QUAN Mingxiu(Institute of Metal Research;The Chinese Academy of Sciences;Shenyang 110015). FORMATION MECHANISM OF NiAl/TiC NANOCOMPOSITE BY MECHANICAL ALLOYING. Acta Metall Sin, 1997, 33(11): 1222-1226.
|
|
|
Abstract Ni, Al, Ti, and C powders mixed at a composition of Ni37Al37Ti37C13 were milled in a high-energy ball mill.Upon milling for 107 min,an abrupt reaction occurred, resulting in in situ formation of NiAl and TiC compounds.The formation mechanism is suggested to be two separated combustion reactions, i.e. Ni+Al→NiAl and Ti+C→TiC. The combustion reaction conducted incompletely and small amount of elemental powders still existed. Prolonged milling led to gradual formation of NiAl and TiC as well as the refinement of grain sizes. The final saturated grain size for TiC is 2.5 times as large as that for NiAl, though TiC has a much higher melting point compared with NiAl, this is attributed to a different deformation mechanism.
|
|
Received: 18 November 1997
|
1MiracleDB.ActaMetallMater,1993;41:649 2NoebeRD,BowmanRR,NathalMV.IntMaterRev,1993;38:193 3HwangSJ,NashP,DollarM,DymekS.MaterSciForum,1992;88—90:611 4KochCC.NanostructMater,1993;2:109 5AtzmonM.PhysRevLett,1990;64:487 6MaE,PaganJ,CranfordG,AtzmonM.JMaterRes,1993;8:1836 7PatankarSN,XiaoSQ,LewandowskiJJ,HeuerAH.JMaterRes,1993;8:1311 8ParkYH,HashimotoH,AbeT,WatanabeR.MaterSciEng,1994;A181/182:1291 9LiuZG,GuoJT,YeLL,LiGS,HuZQ.ApplPhysLett,1994;65:2666 10EckertJ,SchwarzL,HellsternE,UrbanK.JApplPhys,1988;64:3224 11KochCC.AnnRevMaterSci,1989;19:121 12DeeviSC.JMaterSci,1991;26:3343 13LiuZG,GuoJT,LiGS,HuZQ.ActaMetallSin(Engl.Ed),1994;7:7 14BarinI,KnackeO,Kwbashewski.ThermochemicalPropertiesofInorganicSubstances(Supplement).Berlin:Springer-Verlag,1977 15GuoJT,XingZP.JMaterRes,1997;12:1083} |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|