Flow Stress, Microstructural Evolution, and Constitutive Analysis During High-Temperature Deformation in Mg-4.4Li-2.5Zn-0.46Al-0.74Y Alloy
CAO Furong1,2,3(), DING Xin1,4, XIANG Chao1, SHANG Huihui1
1.School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China 2.Key Laboratory of Lightweight Structural Materials Liaoning Province, Northeastern University, Shenyang 110819, China 3.State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819, China 4.Sichuan Aerospace Changzheng Equipment Manufacturing Co. , Ltd. , Chengdu 610000, China
Cite this article:
CAO Furong, DING Xin, XIANG Chao, SHANG Huihui. Flow Stress, Microstructural Evolution, and Constitutive Analysis During High-Temperature Deformation in Mg-4.4Li-2.5Zn-0.46Al-0.74Y Alloy. Acta Metall Sin, 2021, 57(7): 860-870.
Mg-Li alloys have potential applications in the aerospace, military, electronics, and automobile fields due to their superlight density, extremely high specific stiffness, high specific strength, damping, and electromagnetic shielding properties. Due to the limited slip systems of Mg and hcp-structured α(Mg) at room temperature, magnesium and α(Mg)-based alloys are difficult to deform; thus, it is significant to investigate the high-temperature deformation behavior to address this issue. Thus, in this study, an ultralight α(Mg)-based Mg-4.4Li-2.5Zn-0.46Al-0.74Y alloy was fabricated via multi-directional forging and rolling, and its flow stress, microstructural evolution, constitutive modeling, and deformation mechanism at elevated temperatures were investigated by tensile tests, OM, and XRD. The results indicate that the grain refinement mechanism of this alloy processed by multi-directional forging (MDF) exhibits mechanical shearing fragmentation and dynamic recrystallization (DRX). Additionally, the flow stress results demonstrate that strain-hardening occurred at 623 K due to grain coarsening, and microstructural evolution reveals that dynamic recovery and DRX occurred at tensile temperatures of 523-573 K; however, grain coarsening primarily appeared at 573 K (or more). XRD analysis demonstrates that this alloy comprised α(Mg), β(Li), Al2Y, Al12Mg17, LiAl, and Mg2Y phases, and hyperbolic sine constitutive analysis reveals that the stress exponent was 4.4 and the activation energy for deformation was 120.40 kJ/mol. The calculated results for dislocation density, number of dislocations in a grain, and atomic diffusion at 623 K and 1.67 × 10-4 s-1 corresponding to elongation-to-failure of 240% indicate that dislocation creep controlled by lattice diffusion governed the deformation mechanism under this condition. Predictions by grain growth models indicate that the calculated grain sizes were in good agreement with the practical grain sizes at 623 K and 1.67 × 10-4 s-1 when the grain growth factor was equal to 2 and proportional factor was 0.2.
Fig.1 The true stress-true strain curves of Mg-4.4Li-2.5Zn-0.46Al-0.74Y (LZAY4301) alloy at different temperatures and strain rates of 1.67 × 10-2 s-1 (a), 1.67 × 10-3 s-1 (b), 5.0 × 10-4 s-1 (c), and 1.67 × 10-4 s-1 (d)
Fig.2 Microstructures of as-cast (a), MDF 1st pass (b), MDF 3rd pass (c), MDF 6th pass (d), cold-rolled along longitudinal direction (e), and annealed and held at 523 K for 1.25 h (f) in LZAY4301 alloy before high-temperature deformation (MDF—multi-directional forging, DRX—dynamic recrystallization)
Fig.3 XRD spectrum of LZAY4301 alloy annealed at 523 K for 1h
Fig.4 OM images of gauge section in LZAY4301 alloy after high-temperature deformation at temperatures of 523 K (a1-a4), 573 K (b1-b4), and 623 K (c1-c4), and strain rates of 1.67 × 10-2 s-1 (a1-c1), 1.67 × 10-3 s-1 (a2-c2), 5.00 × 10-4 s-1 (a3-c3), and 1.67 × 10-4 s-1 (a4-c4)
Temperature
K
Strain rate
s-1
Grain size
μm
Elongation
%
523
1.67 × 10-2
17.78
144.6
1.67 × 10-3
17.92
147.9
5.00 × 10-4
16.39
202.2
1.67 × 10-4
17.19
189.3
573
1.67 × 10-2
17.59
153.4
1.67 × 10-3
21.23
160.8
5.00 × 10-4
27.64
197.9
1.67 × 10-4
29.33
213.5
623
1.67 × 10-2
23.07
178.3
1.67 × 10-3
29.74
193.8
5.00 × 10-4
32.97
235.0
1.67 × 10-4
34.48
240.0
Table 1 The grains sizes and corresponding elongations of LZAY4301 alloy at different temperatures and strain rates
Fig.5 Curves of ln-lnσ (a), ln-σ (b), ln-ln[sinh(ασ)] (c), and ln[sinh(ασ)]-1 / T (d) of LZAY4301 alloys under high temperature tensile condition (—strain rate, σ—true stress, α—stress multiplier factor, T—absolute temperature; the number adjacent to the regression line indicates specific slope)
Fig.6 Relation curve of lnZ-ln[sinh(ασ)] (a), and comparison of calculated stress and measured stress (b) (Z—Zener-Hollomon parameter, r2—related coefficient)
1
Ji Q, Wang Y, Wu R Z, et al. High specific strength Mg-Li-Zn-Er alloy processed by multi deformation processes [J]. Mater. Charact., 2020, 160: 110135
2
Perugu C S, Kumar S, Suwas S. Evolution of microstructure, texture, and tensile properties in two-phase Mg-Li alloys: Effect of Zn addition [J]. JOM, 2020, 72: 1627
3
Ji H, Wu G H, Liu W C, et al. Microstructure characterization and mechanical properties of the as-cast and as-extruded Mg-xLi-5Zn-0.5Er (x = 8, 10 and 12 wt%) alloys [J]. Mater. Charact., 2020, 159: 110008
4
Guo F, Liu L, Ma Y L, et al. Slip behavior and its effect on rolling texture development in a dual-phase Mg-Li alloy [J]. J. Alloys Compd., 2020, 813: 152117
5
Shah S S A, Wu D, Chen R S, et al. Temperature effects on the microstructures of Mg-Gd-Y alloy processed by multi-direction impact forging [J]. Acta Metall. Sin. (Eng. Lett.), 2020, 33: 243
6
Dong B B, Zhang Z M, Yu J M, et al. Microstructure, texture evolution and mechanical properties of multi-directional forged Mg-13Gd-4Y-2Zn-0.5Zr alloy under decreasing temperature [J]. J. Alloys Compd., 2020, 823: 153776
7
Wei J S, Jiang S N, Chen Z Y, et al. Increasing strength and ductility of a Mg-9Al alloy by dynamic precipitation assisted grain refinement during multi-directional forging [J]. Mater. Sci. Eng., 2020, A780: 139192
8
Kobayashi M, Yoden Y, Aoba T, et al. Microstructure and mechanical properties of multi-directionally-forged AZ80-F magnesium alloys at warm temperatures [J]. J. Jpn. Inst. Met. Mater., 2020, 84: 190
9
Mehrabi A, Mahmudi R, Miura H. Superplasticity in a multi-directionally forged Mg-Li-Zn alloy [J]. Mater. Sci. Eng., 2019, A765: 138274
10
Zhang T L, Tokunaga T, Ohno M, et al. Low temperature superplasticity of a dual-phase Mg-Li-Zn alloy processed by a multi-mode deformation process [J]. Mater. Sci. Eng., 2018, A737: 61
11
Zhou M R, Morisada Y, Fujii H, et al. Pronounced low-temperature superplasticity of friction stir processed Mg-9Li-1Zn alloy [J]. Mater. Sci. Eng., 2020, A780: 139071
12
Cao F R, Zhang J, Ding X, et al. Mechanical properties and microstructural evolution in a superlight Mg-6.4Li-3.6Zn-0.37Al-0.36Y alloy processed by multidirectional forging and rolling [J]. Mater. Sci. Eng., 2019, A760: 377
13
Cao F R, Xue G Q, Xu G M. Superplasticity of a dual-phase-dominated Mg-Li-Al-Zn-Sr alloy processed by multidirectional forging and rolling [J]. Mater. Sci. Eng., 2017, A704: 360
14
Lin Y C, Chen X M. A critical review of experimental results and constitutive descriptions for metals and alloys in hot working [J]. Mater. Des., 2011, 32: 1733
15
Armstrong R W, Li Q Z. Dislocation mechanics of high-rate deformations [J]. Metall. Mater. Trans., 2015, 46A: 4438
16
Barezban M H, Mirzadeh H, Roumina R, et al. Constitutive analysis of wrought Mg-Gd magnesium alloys during hot compression at elevated temperatures [J]. J. Alloys Compd., 2019, 791: 1200
17
Ciccarelli D, El Mehtedi M, Jäger A, et al. Analysis of flow stress and deformation mechanism under hot working of ZK60 magnesium alloy by a new strain-dependent constitutive equation [J]. J. Phys. Chem. Solids, 2015, 87: 183
18
Arun M S, Chakkingal U. A constitutive model to describe high temperature flow behavior of AZ31B magnesium alloy processed by equal-channel angular pressing [J]. Mater. Sci. Eng., 2019, A754: 659
19
Zhang F, Liu Z, Yang M M, et al. Microscopic mechanism exploration and constitutive equation construction for compression characteristics of AZ31-TD magnesium alloy at high strain rate [J]. Mater. Sci. Eng., 2020, A771: 138571
20
Spigarelli S, Jäger A, El Mehtedi M, et al. Microstructural and constitutive analysis in process modeling of hot working: The case of a Mg-Zn-Mn alloy [J]. Mater. Sci. Eng., 2016, A661: 40
21
Xiao B, Xu L Y, Zhao L, et al. Tensile mechanical properties, constitutive equations, and fracture mechanisms of a novel 9% chromium tempered martensitic steel at elevated temperatures [J]. Mater. Sci. Eng., 2017, A690: 104
22
Shalbafi M, Roumina R, Mahmudi R. Hot deformation of the extruded Mg-10Li-1Zn alloy: Constitutive analysis and processing maps [J]. J. Alloys Compd., 2017, 696: 1269
23
Liu G, Xie W, Hadadzadeh A, et al. Hot deformation behavior and processing map of a superlight dual-phase Mg-Li alloy [J]. J. Alloys Compd., 2018, 766: 460
24
Xu T C, Peng X D, Qin J, et al. Dynamic recrystallization behavior of Mg-Li-Al-Nd duplex alloy during hot compression [J]. J. Alloys Compd., 2015, 639: 79
25
Li Y, Guan Y J, Zhai J Q, et al. Hot deformation behavior of LA43M Mg-Li alloy via hot compression tests [J]. J. Mater. Eng. Perform., 2019, 28: 7768
26
Langdon T G. Seventy-five years of superplasticity: Historic developments and new opportunities [J]. J. Mater. Sci., 2009, 44: 5998
27
Kawasaki M, Figueiredo R B, Langdon T G. The requirements for superplasticity with an emphasis on magnesium alloys [J]. Adv. Eng. Mater., 2016, 18: 127
28
Sellars C M, McTegart W J. On the mechanism of hot deformation [J]. Acta Metall., 1966, 14: 1136
29
Mirzadeh H. Developing constitutive equations of flow stress for hot deformation of AZ31 magnesium alloy under compression, torsion, and tension [J]. Int. J. Mater. Form., 2019, 12: 643
30
Zener C, Hollomon J H. Effect of strain rate upon plastic flow of steel [J]. J Appl. Phys., 1944, 15: 22
31
Frost H J, Ashby M F. Deformation-Mechanism Maps [M]. Oxford: Pergamon Press, 1982: 21
32
Cao F R, Xia F, Xue G Q. Hot tensile deformation behavior and microstructural evolution of a Mg-9.3Li-1.79Al-1.61Zn alloy [J]. Mater. Des., 2016, 92: 44
33
Kawasaki M, Kubota K, Higashi K, et al. Flow and cavitation in a quasi-superplastic two-phase magnesium-lithium alloy [J]. Mater. Sci. Eng., 2006, A429: 334
34
Langdon T G, Mohamed F A. A new type of deformation mechanism map for high-temperature creep [J]. Mater. Sci. Eng., 1978, 32: 103
35
Cao F R, Zhou B J, Yin B, et al. Modeling of deformation energy at elevated temperatures and its application in Mg-Li-Al-Y alloy [J]. Trans. Nonferrous Met. Soc. China, 2017, 27: 2434
36
Shah S S A, Wu D, Wang W H, et al. Microstructural evolution and mechanical properties of a Mg-Gd-Y alloy processed by impact forging [J]. Mater. Sci. Eng., 2017, A702: 153
37
Zhang Y, Shao J B, Chen T, et al. Deformation mechanism and dynamic recrystallization of Mg-5.6Gd-0.8Zn alloy during multi-directional forging [J]. Acta Metall. Sin., 2020, 56: 723
Kim W J, Kwak T Y. Constitutive modeling and understanding of the hot compressive deformation of Mg-9.5Zn-2.0Y magnesium alloy with reduced number of strain-dependent constitutive parameters [J]. Met. Mater. Int., 2017, 23: 660
39
Massalski T B, Okamoto H, Subramanian P R, et al. Binary Alloy Phase Diagrams [M]. 2nd Ed., Materials Park, OH: ASM International, 1990: 1
Cao F R, Ding H, Li Y L, et al. Superplasticity, dynamic grain growth and deformation mechanism in ultra-light two-phase magnesium-lithium alloys [J]. Mater. Sci. Eng., 2010, A527: 2335
42
Ruano O A, Wadsworth J, Sherby O D. Deformation mechanisms in an austenitic stainless steel (25Cr-20Ni) at elevated temperature [J]. J. Mater. Sci., 1985, 20: 3735
43
Taleff E M, Ruano O A, Wolfenstine J, et al. Superplastic behavior of a fine-grained Mg-9Li material at low homologous temperature [J]. J. Mater. Res., 1992, 7: 2131
44
Nayeb-Hashemi A A, Clark J B, Pelton A D. The Li-Mg (lithium-magnesium) system [J]. Bull. Alloy Phase Diagr., 1984, 5: 365
45
Sherwood D J, Hamilton C H. A mechanism for deformation-enhanced grain growth in single phase materials [J]. Scr. Metall. Mater., 1991, 25: 2873
46
Cao F R, Lei F, Cui J Z, et al. Modification of a deformation induced grain growth model of superplasticity and its experimental verification [J]. Acta Metall. Sin., 1999, 35: 770