Please wait a minute...
Acta Metall Sin  1997, Vol. 33 Issue (11): 1161-1164    DOI:
Current Issue | Archive | Adv Search |
ADIABATIC SHEAR BAND IN WHITE-ETCHING LAYER
ZHANG Baofa;SHEN Wanci;LIU Yingjie; WANG Yuanfei;TANG Xiangyun (Tsinghua University;Beijing 100084)
Cite this article: 

ZHANG Baofa;SHEN Wanci;LIU Yingjie; WANG Yuanfei;TANG Xiangyun (Tsinghua University;Beijing 100084). ADIABATIC SHEAR BAND IN WHITE-ETCHING LAYER. Acta Metall Sin, 1997, 33(11): 1161-1164.

Download:  PDF(1830KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Adiabatic shear band was observed in surface white-etching layer in impact wear test.The band possesses very fine crystalline grains,and is harder than white-etching layer.The adiabatic shear bnad in white-etching layer is liable to fracture or cracking in impact wear.It's supposed that dynamic recrystallization occures in the band in white-etching layer whereas dynamic recovery takes place in the white-etching layer.
Key words:  white-etching layer      adiabatic shear band      impact wear      dynamic recovery      dynamic recrystallization      fracture     
Received:  18 November 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I11/1161

1ScottD,SmithAI,TaitJ,TremainGR.Wear,1975;33:293
2ZenerC,HollomonJH.JApplPhys,1944;15:22
3BackmanME.FinneganSA.In:PohdeRW,ButcherBM,HollandJR,KarnesCHeds,MetalluryicalEffectsatHighStrainRates,NewYork:Plenum,1973:531
4张保法,刘英杰,沈万慈,王远飞,唐祥云.科学通报,1996;41:374
5ZhangBF,LiuYJ,ShenWC,WangYF,TangXY,WangXD.Wear,1996;198:287
6GriffithsBJ.JTribol,1987;109:525
7BaiYL.ResMech,1990;31:133
8WittmanCL,MeyersMA,PakHR.MetallTrans,1990;21A:707
[1] LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling. Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy[J]. 金属学报, 2023, 59(7): 855-870.
[2] LOU Feng, LIU Ke, LIU Jinxue, DONG Hanwu, LI Shubo, DU Wenbo. Microstructures and Formability of the As-Rolled Mg- xZn-0.5Er Alloy Sheets at Room Temperature[J]. 金属学报, 2023, 59(11): 1439-1447.
[3] WU Jin, YANG Jie, CHEN Haofeng. Fracture Behavior of DMWJ Under Different Constraints Considering Residual Stress[J]. 金属学报, 2022, 58(7): 956-964.
[4] WU Caihong, FENG Di, ZANG Qianhao, FAN Shichun, ZHANG Hao, LEE Yunsoo. Microstructure Evolution and Recrystallization Behavior During Hot Deformation of Spray Formed AlSiCuMg Alloy[J]. 金属学报, 2022, 58(7): 932-942.
[5] GU Ruicheng, ZHANG Jian, ZHANG Mingyang, LIU Yanyan, WANG Shaogang, JIAO Da, LIU Zengqian, ZHANG Zhefeng. Fabrication of Mg-Based Composites Reinforced by SiC Whisker Scaffolds with Three-Dimensional Interpenetrating-Phase Architecture and Their Mechanical Properties[J]. 金属学报, 2022, 58(7): 857-867.
[6] PENG Zichao, LIU Peiyuan, WANG Xuqing, LUO Xuejun, LIU Jian, ZOU Jinwen. Creep Behavior of FGH96 Superalloy at Different Service Conditions[J]. 金属学报, 2022, 58(5): 673-682.
[7] LI Min, LI Haoze, WANG Jijie, MA Yingche, LIU Kui. Effect of Ce on the Microstructure, High-Temperature Tensile Properties, and Fracture Mode of Strip Casting Non-Oriented 6.5%Si Electrical Steel[J]. 金属学报, 2022, 58(5): 637-648.
[8] REN Shaofei, ZHANG Jianyang, ZHANG Xinfang, SUN Mingyue, XU Bin, CUI Chuanyong. Evolution of Interfacial Microstructure of Ni-Co Base Superalloy During Plastic Deformation Bonding and Its Bonding Mechanism[J]. 金属学报, 2022, 58(2): 129-140.
[9] JIANG Weining, WU Xiaolong, YANG Ping, GU Xinfu, XIE Qingge. Formation of Dynamic Recrystallization Zone and Characteristics of Shear Texture in Surface Layer of Hot-Rolled Silicon Steel[J]. 金属学报, 2022, 58(12): 1545-1556.
[10] HU Chen, PAN Shuai, HUANG Mingxin. Strong and Tough Heterogeneous TWIP Steel Fabricated by Warm Rolling[J]. 金属学报, 2022, 58(11): 1519-1526.
[11] FAN Guohua, MIAO Kesong, LI Danyang, XIA Yiping, WU Hao. Unraveling the Strength-Ductility Synergy of Heterostructured Metallic Materials from the Perspective of Local Stress/Strain[J]. 金属学报, 2022, 58(11): 1427-1440.
[12] CHEN Ruirun, CHEN Dezhi, WANG Qi, WANG Shu, ZHOU Zhecheng, DING Hongsheng, FU Hengzhi. Research Progress on Nb-Si Base Ultrahigh Temperature Alloys and Directional Solidification Technology[J]. 金属学报, 2021, 57(9): 1141-1154.
[13] NI Ke, YANG Yinhui, CAO Jianchun, WANG Liuhang, LIU Zehui, QIAN Hao. Softening Behavior of 18.7Cr-1.0Ni-5.8Mn-0.2N Low Nickel-Type Duplex Stainless Steel During Hot Compression Deformation Under Large Strain[J]. 金属学报, 2021, 57(2): 224-236.
[14] ZHOU Hongwei, BAI Fengmei, YANG Lei, CHEN Yan, FANG Junfei, ZHANG Liqiang, YI Hailong, HE Yizhu. Low-Cycle Fatigue Behavior of 1100 MPa Grade High-Strength Steel[J]. 金属学报, 2020, 56(7): 937-948.
[15] YANG Jie, WANG Lei. Effect and Optimal Design of the Material Constraint in the DMWJ of Nuclear Power Plants[J]. 金属学报, 2020, 56(6): 840-848.
No Suggested Reading articles found!