RELATIONSHIP BETWEEN MICROSTRUCTURE AND FATIGUE CRACK PROPAGATION BEHAVIOUR IN TiB_2 PARTICULATE REINFORCED ZA-8 Zn ALLOY
HUA Wenjun(Beijing Institute of Aeronautical Materials; Beijing 100095); WANG Zhirui; ZHANG Jirong( University of Toronto; Canada)(Manuscript received 1 995-06-09; in revised form 1995-1 0-02)
Cite this article: 

HUA Wenjun(Beijing Institute of Aeronautical Materials; Beijing 100095); WANG Zhirui; ZHANG Jirong( University of Toronto; Canada)(Manuscript received 1 995-06-09; in revised form 1995-1 0-02). RELATIONSHIP BETWEEN MICROSTRUCTURE AND FATIGUE CRACK PROPAGATION BEHAVIOUR IN TiB_2 PARTICULATE REINFORCED ZA-8 Zn ALLOY. Acta Metall Sin, 1996, 32(3): 254-260.

Download:  PDF(689KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The relationships between microstructure, fracture surface and propagation behaviour of fatigue crack in TiB2 particulate reinforced ZA-8 Zn alloy and in the corresponding constitute matrix materials were studied. The present results indicate that the resistance to fatigue crack growth of the employed composite is in general superior to that of constitute matrix materials, especially for the short crack behaviour. This is attributed to (1) the interaction between particle and crack tip decreased the stress intensity ahead of the crack tip,(2) owing to the excellent interface strength,(3) the addition of reinforcement caused the change of matrix microstructure and refined the structure and (4) the bridging function of reinforcement. Finally, the mechanism for the difference in fatigue crack growth behaviour of the two materials was discussed. Correspondent HUA Wenjun, Beijing Institute of Aeronautical Materials, Beijing 100095
Key words:  fatigue crack propagation      interface strength      microstructure     
Received:  18 March 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I3/254

1ChinCS,SmithRA.IntJFatikue,1985,7(2):872KumaiShinji,KingJE,KnottJF.FatikueFractEngMaterStruct,1993,15:13RavichandranKS,LarsenJM.MaterSciEng,1992,A153:4994ShangJianKu,RitchieRO.In:EverettRK,ArsenaultRJ,eds,MetalMatrixComposites:MechanismsandProperties,NewYork:Academicpress,1991:2555SureshS.FatigueMater,CambrigeSolidStateScienceSeries,1991,2956WangZhirui,ZhangJirong.MaterSciEng,1993:171:857AtkinsonC.IntJEngSci,1972,10:458KassamZnlfikar,ZhangRJ,WangZhirui.FiniteElementSimulalionofStressDistributtonatCrackTipinParticlesMetalMatrixComposites,UnipublishedResearch,UniversityofToronto,19949KumaiShinji,KingJE,KnottJF.FatigueFractEngMaterStrut,1990,13:511
[1] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[2] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[3] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[4] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[5] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[6] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[7] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[8] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[9] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[10] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[11] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[12] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[13] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[14] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[15] ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui. Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 647-656.
No Suggested Reading articles found!