| MICROTWINNING DEFORMATION IN PST TiAl CRYSTAL |
| LIU Yi; WANG Dening; CHEN Da; LIN Dongliang; (Department of Materials Science; Shanghai Jiaotong University;Shanghai 200030) CHEN Shipu (Shanghai Jiaotong University; Shanghai 200030; State Key Laboratory of Solid State Microstructures of Nanjing University; Nanjing 210008); LIU Zhiyuo (Nanjing University; Nanjing 210008) |
|
Cite this article:
LIU Yi; WANG Dening; CHEN Da; LIN Dongliang; (Department of Materials Science; Shanghai Jiaotong University;Shanghai 200030) CHEN Shipu (Shanghai Jiaotong University; Shanghai 200030; State Key Laboratory of Solid State Microstructures of Nanjing University; Nanjing 210008); LIU Zhiyuo (Nanjing University; Nanjing 210008). MICROTWINNING DEFORMATION IN PST TiAl CRYSTAL. Acta Metall Sin, 1995, 31(9): 393-398.
|
|
|
Abstract The behaviour of microtwinning in TiAl PST crystal has been investigated by TEM. The results show that the microtwinning plane is(111) and microtwin results from the movement of (1/6)[112] Shockley partials. The microtwinning can moved across the twin-related interface of lamellar TiAl phase without changing the twinsystem. These results indicate that the twin-related interface of TiAl can not hinder the microtwinning effectively. The effects of microtwinning on the deformation of PST crystal have been discussed.
|
|
Received: 18 September 1995
|
| 1KimYW,JOM,1989;41:242TsujimotoT,HashimotoK.In:LiuCT,TaubAI,StoloffNS,KochCC,eds.HighTemperatureOrderedIntermetallicAlloysⅢ,MRSSympProc,Pittsburgh,PA:MRSSociety,1989;133:3913HuangSC,HallEJ.ActaMetallMater,1991;39:10534ZhaoLR,TangriK.PhitosMagA,1992;65:10655MorrisMA.PhilosMagA,1993;68:2376FujiwarwT,NakamuraA,HosomiM,nishitauiSR,ShiraiY,YamaguchiM.PhilosMagA,1990;60:5917YamaguchiM,UmakoshiY,ProgrinMaterSci.1990;34:658TunstallWJ,GoodhewPJ.PhitosMag.1966;13:12599ShechtmanD,BlackburnMJ,LipsittHA.MetallTrans.1974;5:137310LipsittHA,ShechtmanD,SchafrikRE.MetallTrans,1975;6:199111HugG,LoiseauA,LasalmonieA.PhijosMagA,1986;54:47 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|