Please wait a minute...
Acta Metall Sin  1995, Vol. 31 Issue (8): 340-345    DOI:
Current Issue | Archive | Adv Search |
A DIFFUSION MODEL IN NANOCRYSTALLINE MATERIALS
CHEN Da(Shanghai Jiaotong University; Shanghai;200030)
Cite this article: 

CHEN Da(Shanghai Jiaotong University; Shanghai;200030). A DIFFUSION MODEL IN NANOCRYSTALLINE MATERIALS. Acta Metall Sin, 1995, 31(8): 340-345.

Download:  PDF(461KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The activation energies,the preexponential factors and the corresponding self-diffusion coefficients for a nanocrystalline material in various diffusion conditions were calculated. Based on comparison of the calculated self-diffusions with the experimentally measured one, it is suggested that the diffusion model in nanocrystals is a complex one with the combination of the boundary diffusion by the vacancy mechanism and the internal surface diffusion of atoms along internal surfaces of boundary voids. CHEN Da, professor, Department of Materials Science, Shanghai Jiaotong University, Shanghai 200030
Key words:  nanocrystalline materials      diffusion      computer modeling     
Received:  18 August 1995     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I8/340

1GleiterH.ProgMaterSci,1989;33:2232BirringerR.MaterSciEng,1989;A117:333HorvathJ,BirringerR,GleiterH.SolidStalComm,1987;62:3194PetersonNL.InterMetRev,1983;28:655BalluffiRW.In:GraemeE,MurchEeds.,DiffusioninCrystallineSolid.Orlando:AcademicPress,1984:3206陈达.金属学报,1994;30:A3487AcklandGJ,TichyG,VitekV,FinnisMW.PhilosMag,1987;56:7358GilmerGH.ComputationalMaterialsScicnce,1994;2:499MurchGE.In:GraemeE,MurchEeds.,DiffusioninCrystallineSolid.Orlando:AcademicPress,1984:37910LeclaireAD.ActaMetall,1953;1:43811ZenerC.JApplPhys,1951;22:37212ZenerC.In:WileyJed.,TheoryofDiffusion,ImperfectionsinNearlyPerfectCrystals,NewYork:AcademicPress,1952:289
[1] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[2] XU Wenguo, HAO Wenjiang, LI Yingju, ZHAO Qingbin, LU Bingyu, GUO Heyi, LIU Tianyu, FENG Xiaohui, YANG Yuansheng. Effects of Trace Aluminum and Titanium on High Temper-ature Oxidation Behavior of Inconel 690 Alloy[J]. 金属学报, 2023, 59(12): 1547-1558.
[3] LIU Lujun, LIU Zheng, LIU Renhui, LIU Yong. Grain Boundary Structure and Coercivity Enhancement of Nd90Al10 Alloy Modified NdFeB Permanent Magnets by GBD Process[J]. 金属学报, 2023, 59(11): 1457-1465.
[4] LI Sai, YANG Zenan, ZHANG Chi, YANG Zhigang. Phase Field Study of the Diffusional Paths in Pearlite-Austenite Transformation[J]. 金属学报, 2023, 59(10): 1376-1388.
[5] SHEN Yingying, ZHANG Guoxing, JIA Qing, WANG Yumin, CUI Yuyou, YANG Rui. Interfacial Reaction and Thermal Stability of the SiCf/TiAl Composites[J]. 金属学报, 2022, 58(9): 1150-1158.
[6] LI Xifeng, LI Tianle, AN Dayong, WU Huiping, CHEN Jieshi, CHEN Jun. Research Progress of Titanium Alloys and Their Diffusion Bonding Fatigue Characteristics[J]. 金属学报, 2022, 58(4): 473-485.
[7] HUA Yu, CHEN Jianguo, YU Liming, SI Yonghong, LIU Chenxi, LI Huijun, LIU Yongchang. Microstructure Evolution and Mechanical Properties of Dissimilar Material Diffusion-Bonded Joint for High Cr Ferrite Heat-Resistant Steel and Austenitic Heat-Resistant Steel[J]. 金属学报, 2022, 58(2): 141-154.
[8] LIU Zhongwu, HE Jiayi. Several Issues on the Development of Grain Boundary Diffusion Process for Nd-Fe-B Permanent Magnets[J]. 金属学报, 2021, 57(9): 1155-1170.
[9] CHEN Shenghu, RONG Lijian. Oxide Scale Formation on Ultrafine-Grained Ferritic-Martensitic Steel During Pre-Oxidation and Its Effect on the Corrosion Performance in Stagnant Liquid Pb-Bi Eutectic[J]. 金属学报, 2021, 57(8): 989-999.
[10] LI Juan, ZHAO Honglong, ZHOU Nian, ZHANG Yingzhe, QIN Qingdong, SU Xiangdong. Diffusion Bonding of CoCrFeNiCu High-Entropy Alloy to 304 Stainless Steel[J]. 金属学报, 2021, 57(12): 1567-1578.
[11] LIU Chenxi, MAO Chunliang, CUI Lei, ZHOU Xiaosheng, YU Liming, LIU Yongchang. Recent Progress in Microstructural Control and Solid-State Welding of Reduced Activation Ferritic/Martensitic Steels[J]. 金属学报, 2021, 57(11): 1521-1538.
[12] WANG Chao, ZHANG Xu, WANG Yumin, YANG Qing, YANG Lina, ZHANG Guoxing, WU Ying, KONG Xu, YANG Rui. Mechanisms of Interfacial Reaction and Matrix Phase Transition in SiCf /Ti65 Composites[J]. 金属学报, 2020, 56(9): 1275-1285.
[13] SUN Zhengyang, YANG Chao, LIU Wenbo. Phase Field Simulations of the Sintering Process of UO2[J]. 金属学报, 2020, 56(9): 1295-1303.
[14] DING Wen, WANG Xiaojing, LIU Ning, QIN Liang. Diffusion Bonding of Copper and 304 Stainless Steel with an Interlayer of CoCrFeMnNi High-Entropy Alloy[J]. 金属学报, 2020, 56(8): 1084-1090.
[15] SUN Zhengyang, WANG Yutian, LIU Wenbo. Phase-Field Simulation of the Interaction Between Pore and Grain Boundary[J]. 金属学报, 2020, 56(12): 1643-1653.
No Suggested Reading articles found!