Please wait a minute...
Acta Metall Sin  1995, Vol. 31 Issue (8): 346-350    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF PHOSPHORUS ON SOLIDIFICATION,ELEMENT SEGREGATION AND η-PHASE PRECIPITATION IN GH 761 ALLOY
SUM Wenru;GUO Shouren; GUO Jianting;LU Dezhong;HU Zhuangqi (Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015)
Cite this article: 

SUM Wenru;GUO Shouren; GUO Jianting;LU Dezhong;HU Zhuangqi (Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015). EFFECT OF PHOSPHORUS ON SOLIDIFICATION,ELEMENT SEGREGATION AND η-PHASE PRECIPITATION IN GH 761 ALLOY. Acta Metall Sin, 1995, 31(8): 346-350.

Download:  PDF(360KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effects of phosphorus content on solidification process, segregation of elements and formation of η-phase in GH 761 alloy were studied by using metallography and electron microprobe.It was found that phosphorus segregates markedly in interdendritic area and lowers extremely the final solidification temperature of the alloy. It aggravates the segregation of Ti and Ni, and relieves the segregation of Mo, B, S and Si.The results also showed that phosphorus obviously enhances the formation of η-phase,but lowers the precipitated temperature of this phase.SUN Wenru, Institute of Metal Research, Chinese Academy of Sciences,Shenyang 110015
Key words:  solidification      segregation       η-phase      superalloy     
Received:  18 August 1995     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I8/346

1王景唐,陈秋,于永田,李谷松.金属学报,1985;21:A4772ChenC,ThompsonRG,DavisDW.In:LoriaEAed.,Superalloy718,625andVariousDerivatives,Pittsburgh:TMS.1991:3373宋余九.金属的晶界与强度.西安:西安交通大学出版社,1987:484郭守仁,卢德忠.金属学报,1991;27:A421
[1] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[2] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[3] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[4] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[5] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[6] CHEN Jia, GUO Min, YANG Min, LIU Lin, ZHANG Jun. Effects of W Concentration on Creep Microstructure and Property of Novel Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1209-1220.
[7] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[8] FENG Qiang, LU Song, LI Wendao, ZHANG Xiaorui, LI Longfei, ZOU Min, ZHUANG Xiaoli. Recent Progress in Alloy Design and Creep Mechanism of γ'-Strengthened Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1125-1143.
[9] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[10] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[11] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[12] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[13] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
[14] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[15] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
No Suggested Reading articles found!