Please wait a minute...
Acta Metall Sin  1995, Vol. 31 Issue (1): 40-46    DOI:
Current Issue | Archive | Adv Search |
EFFECTS OF IMPURITIES AND Ce ON FRACTURE BEHAVIOUR OF 8090 ALLOY SHEETS IN DIFFERENT ORIENTATIONS
MENG Liang;GENG Dongsheng; ZHENG Xiulin(Northwestern Polytechnical University; Xi'an 710072)(Manuscript received 94-05-09)
Cite this article: 

MENG Liang;GENG Dongsheng; ZHENG Xiulin(Northwestern Polytechnical University; Xi'an 710072)(Manuscript received 94-05-09). EFFECTS OF IMPURITIES AND Ce ON FRACTURE BEHAVIOUR OF 8090 ALLOY SHEETS IN DIFFERENT ORIENTATIONS. Acta Metall Sin, 1995, 31(1): 40-46.

Download:  PDF(515KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effects of the impurities and Ce on the fracture behaviour of 8090 alloy sheets were experimentally investigated.Test results show that Fe and Si in 8090 alloy sheets decrease the plane stress fracture toughness in all orientations tested and the crack initiation and propagation resistance in 45°orientation. Na and K decrease the fracture properties in all orientations tested except the crack initiation resistance in T-L orientation.Adding 0.09% Ce into 8090 alloy sheets shows the beneficial effect on the plane stress fracture toughness.The fracture properties of 8090 alloy sheets containing more Fe and Si could be improved by adding 0.28% Ce. The reason behind it may be attributed to that Ce dissolved in a matrix could make the recrystallization microstructure of 8090 alloy sheets more uniform and finer,and reduce the compound particles precipitated along the grain boundaries, which is benefitcal to suppress the tendency of brittle fracture.Correspondent:(MENG Liang,associate professor,Department of Materials Science and Engineering.Northwestern Polytechnical University,Hi'an,710072)
Key words:  Al-Li alloy      impurity      Ce      fracture behaviour     
Received:  18 January 1995     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I1/40

1EnglerO,MizeraJ,DelecroixM,DriverJ.LuckeK.In:PetersM,Winklerp-Jeds.,Aluminium-Lithium,Vo1.Ⅰ.Proc6thAl-LiIntConfOberursel.Germany:DGMInformationsgesellschaftmbH,1992:3072BowenAW,GatenbyKM,McDarmaidDS,PalmerIG.In:PetersM,Winklerp-J.eds.,Aluminium-Lithium,Vol.Ⅰ,Proc6thAl-LiIntConfOberursel,Germany:DGMInformationsgesellschaftmbH,1992:3273VenkateswaraRaoKT,RitcheRO.ScrMetall.1989;23:11294VenkateswaraRaoKT,RitchieRO.ActaMetallMater,1990;38:23095孟亮,张宝昌,田丽,徐伟宏材料工程,1992;(7-9):2256孟亮,张宝昌,梁英,张卫中,田普科,金属学报,1992;28:A1217耿东生,孟亮,高杨.稀有金属材料与工程,1993;22:468WebsterD.MetallTrans.1987;18A:21819盂亮,张宝昌.金属学报,1993;29:B439
[1] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[2] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[3] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
[4] MU Yahang, ZHANG Xue, CHEN Ziming, SUN Xiaofeng, LIANG Jingjing, LI Jinguo, ZHOU Yizhou. Modeling of Crack Susceptibility of Ni-Based Superalloy for Additive Manufacturing via Thermodynamic Calculation and Machine Learning[J]. 金属学报, 2023, 59(8): 1075-1086.
[5] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[6] LIU Wei, CHEN Wanqi, MA Menghan, LI Kailun. Review of Irradiation Damage Behavior of Tungsten Exposed to Plasma in Nuclear Fusion[J]. 金属学报, 2023, 59(8): 986-1000.
[7] SI Yongli, XUE Jintao, WANG Xingfu, LIANG Juhua, SHI Zimu, HAN Fusheng. Effect of Cr Addition on the Corrosion Behavior of Twinning-Induced Plasticity Steel[J]. 金属学报, 2023, 59(7): 905-914.
[8] WANG Furong, ZHANG Yongmei, BAI Guoning, GUO Qingwei, ZHAO Yuhong. First Principles Calculation of Al-Doped Mg/Mg2Sn Alloy Interface[J]. 金属学报, 2023, 59(6): 812-820.
[9] ZHANG Bin, TIAN Da, SONG Zhuman, ZHANG Guangping. Research Progress in Dwell Fatigue Service Reliability of Titanium Alloys for Pressure Shell of Deep-Sea Submersible[J]. 金属学报, 2023, 59(6): 713-726.
[10] WANG Hanyu, LI Cai, ZHAO Can, ZENG Tao, WANG Zumin, HUANG Yuan. Direct Alloying of Immiscible Tungsten and Copper Based on Nano Active Structure and Its Thermodynamic Mechanism[J]. 金属学报, 2023, 59(5): 679-692.
[11] MA Zongyi, XIAO Bolv, ZHANG Junfan, ZHU Shize, WANG Dong. Overview of Research and Development for Aluminum Matrix Composites Driven by Aerospace Equipment Demand[J]. 金属学报, 2023, 59(4): 457-466.
[12] ZHANG Zhefeng, LI Keqiang, CAI Tuo, LI Peng, ZHANG Zhenjun, LIU Rui, YANG Jinbo, ZHANG Peng. Effects of Stacking Fault Energy on the Deformation Mechanisms and Mechanical Properties of Face-Centered Cubic Metals[J]. 金属学报, 2023, 59(4): 467-477.
[13] LI Dianzhong, WANG Pei. Tailoring Microstructures of Metals[J]. 金属学报, 2023, 59(4): 447-456.
[14] XU Linjie, LIU Hui, REN Ling, YANG Ke. Effect of Cu on In-Stent Restenosis and Corrosion Resistance of Ni-Ti Alloy[J]. 金属学报, 2023, 59(4): 577-584.
[15] WANG Jingyang, SUN Luchao, LUO Yixiu, TIAN Zhilin, REN Xiaomin, ZHANG Jie. Rare Earth Silicate Environmental Barrier Coating Material: High-Entropy Design and Resistance to CMAS Corrosion[J]. 金属学报, 2023, 59(4): 523-536.
No Suggested Reading articles found!