| MICROSTRUCTURE OF CAST SiC_p/2024 Al COMPOSITE AND ITS STRENGTHENING MECHANISM |
| LIN Junshan;SHA Min;SHEN Wenrong;LI Pengxing;WU Renjie Shanghai Jiaotong University |
|
Cite this article:
LIN Junshan;SHA Min;SHEN Wenrong;LI Pengxing;WU Renjie Shanghai Jiaotong University. MICROSTRUCTURE OF CAST SiC_p/2024 Al COMPOSITE AND ITS STRENGTHENING MECHANISM. Acta Metall Sin, 1993, 29(9): 81-87.
|
|
|
Abstract Microstructure of the cast SiC_p/2024 Al composites, containing 5, 10, 15 and20 v.-% SiC particles, under peak-aged state and the strengthening mechanism have beenstudied by TEM observation and Vickers hardness measurements. An increase of dislocationdensity in the matrix and slight reduction of subgrain size may be caused by thereinforcement, but the hardness of the matrix increases no more. Tensile tests show that theelastic modulus and work hardening index increase obviously, and the initial flow stress de-creases first and increases afterwards with the increase of volume fraction of SiC particles. It isbelieved that the stress concentration and the deformation constraint by the reinforcementare two main factors in control of the plastic deformation and strengthening of theSiC_p/2024 composite.
|
|
Received: 18 September 1993
|
1 Hirth J P. Scr Metall Mater, 1991; 25: 1 2 Miller W S. Humphreys F J. Str Metall Mater, 1991; 25: 2623 3 Nardone V C, Prewo K M. Scr Metall, 1986; 20: 43 4 Nardone V C. Scr Metall, 1987; 21: 1313 5 Tata M, Arsenault R J. Scr Metall, 1987; 21: 349 6 Bao G, Hutchinson J W, McMeeking R M. Acta Metall Mater, 1991; 39: 1871 7 Vogelsang M, Arsenault R J, Fisher R M. Metall Trans, 1986: 17A: 379 8 Arsenault R J. Shi N. Mater Sci Eng, 1986; 81: 175 9 Arsenault R J, Wang L, Feng C R. Acta Metall Mater, 1991; 39: 47 10 Lin J S, Li P X, Wu R J. Scr Metall Mater. 1993; 28: 281 11 林君山,李鹏兴,吴人洁.金属学报,1992;28:B465 12 Christman T, Suresh S. Acta Metall, 1988; 36: 1691 13 Dutta I, Allen S M, Hafley J L. Metall Trans, 1991; 22A: 2553 14 Arsenault R J. Mater Sci Eng, 1984; 64: 171 15 Papazian J M, Adler P. N. Metall Trans, 1990; 21A: 401 16 Aikin R M, Christodoulou L. Scr Metall Mater, 1991; 25: 9 17 李中华,王永兰,罗景华,匡震邦,邵谭华,周惠久.金属学报,1987;23:A103 |
| No Suggested Reading articles found! |
|
|