Please wait a minute...
Acta Metall Sin  1993, Vol. 29 Issue (8): 49-54    DOI:
Current Issue | Archive | Adv Search |
ACTIVITY OF DISSOLVED La IN LIQUID Al
XIAO Lisheng;SUI Zhitong;WANG Changzhen Northeast University of Technoiogy; Shengyangprofessor; Department of Metallurgical Physical Chemistry;Northeast University of Technology;Shenyang 110006
Cite this article: 

XIAO Lisheng;SUI Zhitong;WANG Changzhen Northeast University of Technoiogy; Shengyangprofessor; Department of Metallurgical Physical Chemistry;Northeast University of Technology;Shenyang 110006. ACTIVITY OF DISSOLVED La IN LIQUID Al. Acta Metall Sin, 1993, 29(8): 49-54.

Download:  PDF(509KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The rare earth La sensors were made by using polycrystallineLa_(0.95)Ca_(0.05)F_(2.95) as solid electrolyte, LaNi_5-Ni as reference electrode and Mo wire as leadwire. And the activity of dissolved La was directly determined with different La concentra-tions in molten Al at 1023 K. The results were in agreement with that of oxygen concentrationcell EMF determined by oxygen sensors. Some thermodynamic data of Al-La system at1023 K were obtained as follows: △G°_(La)=-175.2 kJ/mol, γ°_(La(s) = 5,85×l0~(-7) ε_(La)~(La)= 28.7, e_(La)~(La)=0.024
Key words:  sensor      activity      La      Al liquid solution     
Received:  18 August 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I8/49

1 Colin J. Smithells, Metals Reference Book, Vol.1, London Butterworths, 1962.
2 肖理生,于化龙,王常珍,徐秀光,1991年冶金学科青年学术交流会论文集,1991:106
3 Fruehan R J. Metall Trans, 1974; 5: 345
4 Gustafsson S, Mellberg D O. Scandinavian J Metall, 1980: 9: 111
5 Mclean A, Bell H. J Iron Steel Inst, 1965; February: 123
6 Janke D., Fisher W A, Arch Eisenhuttenw, 1973; 44: 15
7 孙运涌,杜挺,金属学报,待发表.
8 Dewing Ernest W, Desclaux Paul, Metall Trans, 1990; 21: 861
9 Wang Changzhen, Xu Xiuguang, Man Hauyuan, Xiao Yanping, Inorganica Chimica Acta, 1987; 140: 181A
[1] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
[2] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[3] CHEN Jia, GUO Min, YANG Min, LIU Lin, ZHANG Jun. Effects of W Concentration on Creep Microstructure and Property of Novel Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1209-1220.
[4] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[5] ZHANG Haifeng, YAN Haile, FANG Feng, JIA Nan. Molecular Dynamic Simulations of Deformation Mechanisms for FeMnCoCrNi High-Entropy Alloy Bicrystal Micropillars[J]. 金属学报, 2023, 59(8): 1051-1064.
[6] MU Yahang, ZHANG Xue, CHEN Ziming, SUN Xiaofeng, LIANG Jingjing, LI Jinguo, ZHOU Yizhou. Modeling of Crack Susceptibility of Ni-Based Superalloy for Additive Manufacturing via Thermodynamic Calculation and Machine Learning[J]. 金属学报, 2023, 59(8): 1075-1086.
[7] XU Yongsheng, ZHANG Weigang, XU Lingchao, DAN Wenjiao. Simulation of Deformation Coordination and Hardening Behavior in Ferrite-Ferrite Grain Boundary[J]. 金属学报, 2023, 59(8): 1042-1050.
[8] LIU Wei, CHEN Wanqi, MA Menghan, LI Kailun. Review of Irradiation Damage Behavior of Tungsten Exposed to Plasma in Nuclear Fusion[J]. 金属学报, 2023, 59(8): 986-1000.
[9] WANG Zongpu, WANG Weiguo, Rohrer Gregory S, CHEN Song, HONG Lihua, LIN Yan, FENG Xiaozheng, REN Shuai, ZHOU Bangxin. {111}/{111} Near Singular Boundaries in an Al-Zn-Mg-Cu Alloy Recrystallized After Rolling at Different Temperatures[J]. 金属学报, 2023, 59(7): 947-960.
[10] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[11] SI Yongli, XUE Jintao, WANG Xingfu, LIANG Juhua, SHI Zimu, HAN Fusheng. Effect of Cr Addition on the Corrosion Behavior of Twinning-Induced Plasticity Steel[J]. 金属学报, 2023, 59(7): 905-914.
[12] ZHANG Lu, YU Zhiwei, ZHANG Leicheng, JIANG Rong, SONG Yingdong. Thermo-Mechanical Fatigue Cycle Damage Mechanism and Numerical Simulation of GH4169 Superalloy[J]. 金属学报, 2023, 59(7): 871-883.
[13] LI Qian, LIU Kai, ZHAO Tianliang. Rust Formation Behavior and Mechanism of Q235 Carbon Steel in 5%NaCl Salt Spray Under Elastic Tensile Stress[J]. 金属学报, 2023, 59(6): 829-840.
[14] HOU Juan, DAI Binbin, MIN Shiling, LIU Hui, JIANG Menglei, YANG Fan. Influence of Size Design on Microstructure and Properties of 304L Stainless Steel by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 623-635.
[15] ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui. Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 647-656.
No Suggested Reading articles found!