Acta Metall Sin  1993, Vol. 29 Issue (8): 55-60    DOI:
Current Issue | Archive | Adv Search |
REDUCTION OF CaO-SiO2-Fe_tO TERNARY SLAG BY CO
YANG Xuemin;WANG Daguang;XUAN Demao Institute of Chemical Metallurgy; Academia Sinica; BeijingDepartment No.2;Institute of Chemical Metallurgy;Academia Sinica; Beijing 100080
Cite this article: 

YANG Xuemin;WANG Daguang;XUAN Demao Institute of Chemical Metallurgy; Academia Sinica; BeijingDepartment No.2;Institute of Chemical Metallurgy;Academia Sinica; Beijing 100080. REDUCTION OF CaO-SiO2-Fe_tO TERNARY SLAG BY CO. Acta Metall Sin, 1993, 29(8): 55-60.

Download:  PDF(430KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Apparent reduction rate constant, K_a, was determined by measuringCO_2 evolution with an infrared gas analyser. The relationship between K_a and Fe_tO in slagwas found to be parabolic. K_a approaches to the minimum when either the slag basicity,R<1.0 or=1.5 and Fe_tO content 50% or 70%,respectively. The activities of Fe_tO in CaO-SiO_2- Fe_tO ternary slag system at 1723 K may be calculated by using regular solution model.
Key words:  CaO-SiO_2-Fe_tO system      reduction      activity      reduction rate     
Received:  18 August 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I8/55

1 Nagasaka T, Iguchi Y, Ban--Ya S. Fifth International Iron and Steel Congress, April 6--9,1986; Washington,D.C.U.S.A.
2 Fine H A,Meyer D,Janke D,Engel H-J. Ironmaking and Steelmaking. 1985; 12(4) : 157
3 杨学民,王大光,宣德茂,唐武成.第八届全国冶金物理化学学术研讨会论文集,苏州,1992:153
4 杨学民,王大光,宣德茂,刘天中.冶金学科青年学术交流会论文集,沈阳,1991
5 杨学民,王大光,宣德茂.化工冶金,1993;14:139
6 杨学民,王大光,宣德茂.化工冶金,待发表
7 陈稼祥 编著.炼钢常用图表手册.北京:冶金工业出版社,1984:150,635
8 陈襄武.钢铁冶金物理化学.北京:冶金工业出版社,1990:51
9 Lumsden J. Physical Chemistry of Process Metallurgy, Part Ⅰ. New York: Interscience, 1961: 165
10 Turkdogan E T. Physicochemsitry of Molten Slags and Glasses, London, The Metal Socity 1983
11 万谷志郎,日野光兀.铁钢,1987;73:476H
[1] JU Tianhua, SHU Nian, HE Wei, DING Xueyong. A Predicted Model for Activity Interaction Coefficient Between Solutes in Alloy Solutions[J]. 金属学报, 2023, 59(11): 1533-1540.
[2] WANG Fuqiang, LIU Wei, WANG Zhaowen. Effect of Local Cathode Current Increasing on Bath-Metal Two-Phase Flow Field in Aluminum Reduction Cells[J]. 金属学报, 2020, 56(7): 1047-1056.
[3] XU Shuai, SUN Xinjun, LIANG Xiaokai, LIU Jun, YONG Qilong. Effect of Hot Rolling Deformation on Microstructure and Mechanical Properties of a High-Ti Wear-Resistant Steel[J]. 金属学报, 2020, 56(12): 1581-1591.
[4] Yongli JIN,Hai YU,Jieyu ZHANG,Zengwu ZHAO. Effects of Magnetic Field on Reduction of CaOContaining Iron Oxides[J]. 金属学报, 2019, 55(3): 410-416.
[5] Rongyao MA, Lin ZHAO, Changgang WANG, Xin MU, Xin WEI, Junhua DONG, Wei KE. Influence of Hydrostatic Pressure on the Thermodynamics and Kinetics of Metal Corrosion[J]. 金属学报, 2019, 55(2): 281-290.
[6] Muqin LI, Haitao YAO, Fanghong WEI, Mingda LIU, Zan WANG, Shuhao PENG. The Microstructure and in Vivo and in Vitro Property of Multi-Component Composite Films on the Biomedical Pure Magnesium Surface[J]. 金属学报, 2017, 53(10): 1337-1346.
[7] Xiaofeng LU, Ming XIAO, Yangmei CHEN, Bangcheng YANG. Bioactivity of Titanium Metal Hybridized with Inactivated Bacterial Biofilm[J]. 金属学报, 2017, 53(10): 1402-1412.
[8] Xiaoyan CHEN,Zhe JIN,Xuefeng BAI,Yizhou ZHOU,Tao JIN,Xiaofeng SUN. EFFECT OF C ON THE INTERFACIAL REACTION AND WETTABILITY BETWEEN A Ni-BASED SUPERALLOY AND CERAMIC MOULD[J]. 金属学报, 2015, 51(7): 853-858.
[9] Dongsong RONG,Yong JIANG,Jianming GONG. EXPERIMENTAL RESEARCH AND THERMODYNAMIC SIMULATION OF LOW TEMPERATURE COLOSSAL CARBURIZATION OF AUSTENITIC STAINLESS STEEL[J]. 金属学报, 2015, 51(12): 1516-1522.
[10] DAI Wenbin WANG Xinli YU Jingkun ZOU Zongshu. PRODUCTION OF MgAlON BY CARBOTHERMAL REDUCTION AND NITRIDATION[J]. 金属学报, 2011, 47(11): 1440-1444.
[11] LV Dongsheng; LI Weishan; TAN Chunlin; ZE Ronghua. PREPARATION AND ELECTROCHEMICAL BEHAVIORS OF Co-B ALLOY POWDERS[J]. 金属学报, 2010, 46(3): 346-351.
[12] LIN Qiyong ZHU Miaoyong. INFLUENCE OF CASTING SPEED ON SOFT REDUCTION GRADIENT IN CONTINUOUS CASTING BLOOM[J]. 金属学报, 2009, 45(2): 253-256.
[13] ;. Investigation on Preparation of Tb2Fe17 by Direct Electrochemical Reduction of Tb4O7-Fe2O3 Pellet in Molten Calcium Chloride[J]. 金属学报, 2008, 44(7): 859-862 .
[14] WU Ling. The improvement of regular solution model based on GA-NN and its application in binary slag system[J]. 金属学报, 2008, 44(7): 799-802 .
[15] Yuan Liu. Improvement of Calculation Method for the Activity Coefficient of Multi-component Alloys[J]. 金属学报, 2007, 43(5): 503-508 .
No Suggested Reading articles found!