SOLIDIFIED PRODUCT FROM Bi-Sr-Ca-Cu-O MELT AND ITS TRANSFORMATION INTO SUPERCONDUCTOR
HU Zhuangqi;GE Yunlong;WANG Yongzhong;QIAO Guiwe Institute of Metal Research; Academia Sinica; ShenyangZHANG Cheng;Institute of Metal Research;Academia Sinica ;Shenyang 110015
Cite this article: 

HU Zhuangqi;GE Yunlong;WANG Yongzhong;QIAO Guiwe Institute of Metal Research; Academia Sinica; ShenyangZHANG Cheng;Institute of Metal Research;Academia Sinica ;Shenyang 110015. SOLIDIFIED PRODUCT FROM Bi-Sr-Ca-Cu-O MELT AND ITS TRANSFORMATION INTO SUPERCONDUCTOR. Acta Metall Sin, 1993, 29(5): 41-48.

Download:  PDF(888KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The Bi_2(Sr, Ca)_3Cu_2O_x system superconductor was prepared by different melt-ing procedures and after treatment. The effects of cooling rate, annealing temperature andtime, as well as melting procedures on phase transformation were investigated. The structureand properties were examined by X-ray diffraction, optical microscopy, EPMA, DTA, TGAand measurements of electric and magnetic properties. When the melt of nominal composition Bi_2(Sr, Ca)_3Cu_2O_x solidified in air, the Bi_2(Sr, Ca)_3Cu_2O_(8+δ)(2212) superconductive phaseis stable, the easily solidified product including Bi_2(Sr, Ca)_2CuO_(6+δ)(2201) phase is metas-table, and another may by amorphous if rapidly quenched. The last two may be transformedinto 2212 phase by after treatment with an optimal annealing temperature ranging 780-870℃. While 2201 phase, prepared by the laser floating zone melting method, may easily betransformed into 2212 phase with layer or filament in shape which is favourable to improvethe links among superconductive grains and critic current density.
Key words:  Bi system superconductor      melt      stability      phase transformation     
Received:  18 May 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I5/41

1 Torrance J B, Tokura Y, Laplaca S J, Huang T C, Savog R J. Solid State Commun, 1988; 66: 703
2 Tarason J M, Lepage Y, Greene L H, Bagley B G, Barboux P, Huang D M, Hull G W, McKinnan W R, Giroud M. Phys Rev, 1988; B38: 2504
3 Takei H, Koike M, Takeya H, Suzuki K, Ichihara M. Jpn J Appl Phys, 1989; 28: 1193
4 Liu R S, Huang Y T, Jiang J M, Wu P T, Chang C. Jpn J Appl Phys, 1989; 28: 395
5 Gazit D, Peszkin P N, Moulton L V, Feigelson R S. J Cryst Growth, 1989; 98: 545
6 Oka Y, Yamamoto N, Tomii Y, Kitaguchi H, Oda K, Takada J. Jpn J Appl Phys, 1989; 28: 801
7 Zhang Cheng, Zhang Jishan, Ge Yunlong, Hu Zhuangqi. Chin J Met Sci Technol. 1991; 5: 353
8 Bock J, Preisler E. In: Freyhardt H C, Flukiger R, Peuckert M eds., High-Temperature
Superconductors Materials Aspects, Vol. Ⅰ, Oberursel, FRG: DGM Informationsgesellschaft mbH, 1991: 215
9 Oka Y, Yamamoto N, Kitaguchi H, Oda K, Takada J. Jpn J Appl Phys, 1989; 28: 213
10 Zhang Cheng, Wang Xin, Jiang Ming, Huang Jianguo, Wang Yongzhong, Qiao Guiwen. J Mater Sci Technol, to be poblished
11 Gazit D, Feigelson R S. J Cryst Growth, 1988; 91: 318
12 Lu Z, Moulton L V, Feigelson R S. J Cryst Growth, 1990; 106: 732
13 Lin W J, Wang L C, Lu H B, Lin I N, Young C C, Lin W Y, Yang S J, Hsu S E. Jpn J Appl Phys. 1990; 29: 846
14 郭继延.物理测试,1989;(4) :12
15 乔桂文,王欣.全国高温超导学术讨论会论文集,合肥,1991:34
16 Chaudhari P. J Phys, 1989; C162: 1603
[1] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[2] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[3] DU Jinhui, BI Zhongnan, QU Jinglong. Recent Development of Triple Melt GH4169 Alloy[J]. 金属学报, 2023, 59(9): 1159-1172.
[4] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[5] YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying. Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating[J]. 金属学报, 2023, 59(7): 961-968.
[6] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[7] FENG Li, WANG Guiping, MA Kai, YANG Weijie, AN Guosheng, LI Wensheng. Microstructure and Properties of AlCo x CrFeNiCu High-Entropy Alloy Coating Synthesized by Cold Spraying Assisted Induction Remelting[J]. 金属学报, 2023, 59(5): 703-712.
[8] HOU Juan, DAI Binbin, MIN Shiling, LIU Hui, JIANG Menglei, YANG Fan. Influence of Size Design on Microstructure and Properties of 304L Stainless Steel by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 623-635.
[9] ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui. Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 647-656.
[10] WU Xinqiang, RONG Lijian, TAN Jibo, CHEN Shenghu, HU Xiaofeng, ZHANG Yangpeng, ZHANG Ziyu. Research Advance on Liquid Lead-Bismuth Eutectic Corrosion Resistant Si Enhanced Ferritic/Martensitic and Austenitic Stainless Steels[J]. 金属学报, 2023, 59(4): 502-512.
[11] TANG Weineng, MO Ning, HOU Juan. Research Progress of Additively Manufactured Magnesium Alloys: A Review[J]. 金属学报, 2023, 59(2): 205-225.
[12] WANG Hu, ZHAO Lin, PENG Yun, CAI Xiaotao, TIAN Zhiling. Microstructure and Mechanical Properties of TiB2 Reinforced TiAl-Based Alloy Coatings Prepared by Laser Melting Deposition[J]. 金属学报, 2023, 59(2): 226-236.
[13] WANG Chongyang, HAN Shiwei, XIE Feng, HU Long, DENG Dean. Influence of Solid-State Phase Transformation and Softening Effect on Welding Residual Stress of Ultra-High Strength Steel[J]. 金属学报, 2023, 59(12): 1613-1623.
[14] ZHANG Limin, LI Ning, ZHU Longfei, YIN Pengfei, WANG Jianyuan, WU Hongjing. Macrosegregation Mechanism of Primary Silicon Phase in Cast Hypereutectic Al-Si Alloys Under Alternating Electropulsing[J]. 金属学报, 2023, 59(12): 1624-1632.
[15] ZHANG Kaiyuan, DONG Wenchao, ZHAO Dong, LI Shijian, LU Shanping. Effect of Solid-State Phase Transformation on Stress and Distortion for Fe-Co-Ni Ultra-High Strength Steel Components During Welding and Vacuum Gas Quenching Processes[J]. 金属学报, 2023, 59(12): 1633-1643.
No Suggested Reading articles found!