Abstract A decomposed triphase mixture NdH_2, α-Fe and Fe_2B, sized about 0.1μm,occurred in the matrix Nd_2Fe_(14)B of ingot after hydriding and the Nd_2Fe_(14)B phase of about 0.3.μm re-associated as dehydriding. The Nd-rich boundary phase, distributed around the ma-trix, in the ingot may diffuse into Nd_2Fe_(14)B matrix during hydriding. It shall remain asdehydriding and distributes homogeneously around some colonies composed of fine grains ofNd_2Fe_(14)B.
|
|
Received: 18 May 1993
|
1 Croat J J, Herbst J F, Lee R W, Pinkerton F E. J Appl Phys, 1984; 55: 2078 2 Takeshita T, Nakayana R. Proc of the 10th International Workshop on Rare-Earth Magnets and their Application. Kyoto, Japan, 16--19 May, 1989: 551 3 Nakayama R, Takeshita T, Hakura M, kawano N. Oki K. J Appl Phys, 1991; 70: 3770 4 McGuiness P J, Zhang X J, Yin X J, Harris I R. J Less-Common Met, 1990; 156: 359 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|