EFFECT OF CRYSTALLIZATION ON ACTIVATED DISSOLUTION BEHAVIOUR OF AMORPHOUS FeNiSiB ALLOYS
LI Ying;SONG Guangling;CAO Chunan;LIN Haichao Corrosion Science Laboratory; Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang
Cite this article: 

LI Ying;SONG Guangling;CAO Chunan;LIN Haichao Corrosion Science Laboratory; Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang. EFFECT OF CRYSTALLIZATION ON ACTIVATED DISSOLUTION BEHAVIOUR OF AMORPHOUS FeNiSiB ALLOYS. Acta Metall Sin, 1993, 29(11): 74-78.

Download:  PDF(446KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The corrosion behaviour of FeNiSiB amorphous alloys under different heattreatments has been studied by potentiodynamic polarization method and impedencemeasurement system. The dissolution activity of FeNiSiB amorphous alloys with differentcrystallization states is dependent upon the difference in their phase contents.
Key words:  FeNiSiB amorphous alloy      crystallization      dissolution activity     
Received:  18 November 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I11/74

1 卢博基主编,柯成,唐与堪,罗阳,何开元译.非晶态金属合金.北京:冶金工业出版社,1989:636
2 Archer M D, Corke C C, Harll B H. Electrochem Acta, 1987; 32: 13
3 林栋梁,邹龙飞,吕忆诚.中国腐蚀与防护学报,1988;8:281
4 范耀檀,浦桂根,刘同钧,俞龙飞.中国腐蚀与防护学报,1981;1:10
5 陈晓怡,郭大侠,罗源.金属学报,1988;24:B136
6 刘让苏.国外金属材料,1987;1:40
7 Sorensen N R, Diegl R B, Pieraux S T. Corros Sci, 1987; 40: 2
8 孙中子,王井银.金属学报,1988;24:B68
9 Heusler K E, Huerta D. J Electrochem Soc. 1989; 136: 65
[1] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[2] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[3] LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling. Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy[J]. 金属学报, 2023, 59(7): 855-870.
[4] LOU Feng, LIU Ke, LIU Jinxue, DONG Hanwu, LI Shubo, DU Wenbo. Microstructures and Formability of the As-Rolled Mg- xZn-0.5Er Alloy Sheets at Room Temperature[J]. 金属学报, 2023, 59(11): 1439-1447.
[5] WU Caihong, FENG Di, ZANG Qianhao, FAN Shichun, ZHANG Hao, LEE Yunsoo. Microstructure Evolution and Recrystallization Behavior During Hot Deformation of Spray Formed AlSiCuMg Alloy[J]. 金属学报, 2022, 58(7): 932-942.
[6] GUO Lu, ZHU Qianke, CHEN Zhe, ZHANG Kewei, JIANG Yong. Non-Isothermal Crystallization Kinetics of Fe76Ga5Ge5B6P7Cu1 Alloy[J]. 金属学报, 2022, 58(6): 799-806.
[7] LI Jinfu, LI Wei. Structure and Glass-Forming Ability of Al-Based Amorphous Alloys[J]. 金属学报, 2022, 58(4): 457-472.
[8] REN Shaofei, ZHANG Jianyang, ZHANG Xinfang, SUN Mingyue, XU Bin, CUI Chuanyong. Evolution of Interfacial Microstructure of Ni-Co Base Superalloy During Plastic Deformation Bonding and Its Bonding Mechanism[J]. 金属学报, 2022, 58(2): 129-140.
[9] ZHANG Jinyong, ZHAO Congcong, WU Yijin, CHEN Changjiu, CHEN Zheng, SHEN Baolong. Structural Characteristic and Crystallization Behavior of the (Fe0.33Co0.33Ni0.33)84 -x Cr8Mn8B x High-Entropy-Amorphous Alloy Ribbons[J]. 金属学报, 2022, 58(2): 215-224.
[10] JIANG Weining, WU Xiaolong, YANG Ping, GU Xinfu, XIE Qingge. Formation of Dynamic Recrystallization Zone and Characteristics of Shear Texture in Surface Layer of Hot-Rolled Silicon Steel[J]. 金属学报, 2022, 58(12): 1545-1556.
[11] HU Chen, PAN Shuai, HUANG Mingxin. Strong and Tough Heterogeneous TWIP Steel Fabricated by Warm Rolling[J]. 金属学报, 2022, 58(11): 1519-1526.
[12] HAN Luhui, KE Haibo, ZHANG Pei, SANG Ge, HUANG Huogen. Kinetic Crystallization Behavior of Amorphous U60Fe27.5Al12.5 Alloy[J]. 金属学报, 2022, 58(10): 1316-1324.
[13] JIANG Jufu, ZHANG Yihao, LIU Yingze, WANG Ying, XIAO Guanfei, ZHANG Ying. Research on AlSi7Mg Alloy Semi-Solid Billet Fabricated by RAP[J]. 金属学报, 2021, 57(6): 703-716.
[14] LI Yanmo, GUO Xiaohui, CHEN Bin, LI Peiyue, GUO Qianying, DING Ran, YU Liming, SU Yu, LI Wenya. Microstructure and Mechanical Properties of Linear Friction Welding Joint of GH4169 Alloy/S31042 Steel[J]. 金属学报, 2021, 57(3): 363-374.
[15] NI Ke, YANG Yinhui, CAO Jianchun, WANG Liuhang, LIU Zehui, QIAN Hao. Softening Behavior of 18.7Cr-1.0Ni-5.8Mn-0.2N Low Nickel-Type Duplex Stainless Steel During Hot Compression Deformation Under Large Strain[J]. 金属学报, 2021, 57(2): 224-236.
No Suggested Reading articles found!