KINETICS OF AUSTENITIC ISOTHERMAL DECOMPOSITION AND Mn PARTITION IN Fe-C-Mn-B ALLOYS |
YANG Liu;FANG Hongsheng;MENG Zhihe Southwestern Jiaotong university; Chengdu; Tsinghua University; Beijing; Luoyang Institute of Technology |
|
Cite this article:
YANG Liu;FANG Hongsheng;MENG Zhihe Southwestern Jiaotong university; Chengdu; Tsinghua University; Beijing; Luoyang Institute of Technology. KINETICS OF AUSTENITIC ISOTHERMAL DECOMPOSITION AND Mn PARTITION IN Fe-C-Mn-B ALLOYS. Acta Metall Sin, 1992, 28(1): 16-20.
|
Abstract A proper addition of Mn to Fe--C alloys could delay the isothermal transforma-tion and change the shape of the TTT curves of the alloys. The concentration of Mn at α/γ in-terfaces and their neighboring matrix were measured by STEM / EDAX. The results show that the partition of Mn between α and γ occurs at higher temperature but not at lower temperature. There exists certain temperature range with the strongest Mn concentration spike at the inter-face even though Mn partition between α and γ is not found at the temperature on range. The fact that temperature at which the highest Mn concentration spike occurs is correspondent with the bay temperature on TTT curves shows that the change of TTT curve shape is due to the solute drag effect and solute drag--like effect which are caused by the enrichment of Mn at the α/γ interface.
|
Received: 18 January 1992
|
1 Coates D E. Metall Trans, 1973; 4A: 2313 2 Hillert M. Internal Report, Swedish Institute Metal research, 1953 3 Kirkaldy J S. Can J Phys, 1958; 36: 907 4 Purdy G R, Weichert D H, Kirkaldy J S. Trans Metall Soc AIME, 1964; 230: 1025 5 Hultgren A. Trans ASM, 1947; 39: 915 6 Darken L S. Trans Metall Soc AIME, 1961; 221: 654 7 Aaronson H I, Domian H A. Trans Metall Soc AIME, 1966; 236: 781 8 Gilmour J B, Purdy G R, Kirkaldy J S. Metall Trans, 1972; 3A: 3213 9 Romig A D Jr., Salzbrenner R. Scr Metall, 1982; 16: 33 10 Enomoto M, Aaronson HI. Metall Trans, 1987; 18A: 1547 11 杨柳,方鸿生,陈南平.清华大学学报(自然科学版),1988;28(2) :93 12 Balluffi R W. In: Johnson W C, Blakely J M eds., Interfacial Segregation, Metals Park, Ohio: ASM, 1979: 193 13 Bradley J R, Aaronson H I. Metall Trams, 1981; 12A: 1729 14 Kinsman K R, Aaronson H I. Transformation and hardenability in Steels, Symposium, Ann Arbor, Michigan: Climax Molybdenum Company of Michigan, 1977: 3 |