TEM STUDY ON MICROSTRUCTURE OF A LASERGLAZED SINGLE CRYSTAL Ni-BASE SUPERALLOY |
WANG Huaming;ZHANG Jinghua;TANG Yajun;LI Ying'ao;HU Zhuangqi Institute of Metal Research; Academia Sinica; Shenyang Manuscript received 28 November; 1990; revised manuscript 10 January; 1991 |
|
Cite this article:
WANG Huaming;ZHANG Jinghua;TANG Yajun;LI Ying'ao;HU Zhuangqi Institute of Metal Research; Academia Sinica; Shenyang Manuscript received 28 November; 1990; revised manuscript 10 January; 1991. TEM STUDY ON MICROSTRUCTURE OF A LASERGLAZED SINGLE CRYSTAL Ni-BASE SUPERALLOY. Acta Metall Sin, 1991, 27(6): 9-13.
|
Abstract The microstructure of a rapidly solidified single crystal Ni-base superalloy treated by laserglazing has been observed by TEM and STEM-EDAX techniques.Various morphologies of extraordinary flower-like MC carbide (TiC) were revealed in the narrow interdendritic regiom. While the superfine γ' precipitate and higher density.of dislocation were found in the γmatrix.
|
Received: 18 June 1991
|
1 Breinan E M, Kear B H. In: Bass M ed, Laser Materials Processing, New York: North-Holland, 1983: 235--295 2 Snow D B, Breinan E M, Kear B H. In: Tien J K, Wlodek S T, Morrow H III, Gell M, Maurer G E eds., Superalloys 1980, Metals Park, Ohio: ASM, 1980: 189--194 3 Hu Zhuangqi, Ge Yunlong, Jiang Ming, Jiang Xiaoping, Zhao Qi, Zhang Jishan. Chin J Met Sci Technol, 1988; 4: 134--145 4 Zhao Qi, Hu Zhuangqi, Ge Yunlong, Jiang Ming, Shi Changxu. Chin J Met Sci Technol, 1986; 2: 254--259 5 张静华,唐亚俊,张志亚,李英傲,于洋,张济山,胡壮麒.材料科学进展,1990;4:392-397 6 Strutt P R, Lewis B G, Kear B H. Rapidly Solidified Amorphous and Crystalline Alloys, Proceedings of MRS Annual Meeting, 1981, New York: North-Holland, 1982: 485--498 7 刘林.西北工业大学博士学位论文,1988 8 Fernandez R, Lecomte J C, Kattamis T Z. Metall Trans, 1978; 9A: 1381u |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|