MICROSTRUCTURE AND SOLID SOLUBILITY OF RAPIDLY SOLIDIFIED Ag-Tb ALLOY |
NING Yuantao;ZHOU Xinming;LI Yongnian Kunming Institute of Precious Metals |
|
Cite this article:
NING Yuantao;ZHOU Xinming;LI Yongnian Kunming Institute of Precious Metals. MICROSTRUCTURE AND SOLID SOLUBILITY OF RAPIDLY SOLIDIFIED Ag-Tb ALLOY. Acta Metall Sin, 1990, 26(5): 147-149.
|
Abstract The 0.05--0.08mm thick splat foils of Ag-Tb alloy, containing Tb up to 10 at.-%,were made by the hammer-anvil technique. The cooling rate was in order of 10~6K/s. The me-tastable extension of solid solubility of Tb in the rapidly solidified Ag-Tb alloy was measuredto be up to 5 at.-% by lattice paramter method. The secondary phase in metastable eutecticstructure was identified as Ag_3Tb from diffraction pattern. The microstructure and micro-defect in as-quenched Ag-Tb splat foil were also observed.
|
Received: 18 May 1990
|
1 宁远涛,郑云.金属学报,1983;19:B225 2 Jones H. J Mater Sci, 1984; 19: 1043 3 Gschneidner K A Jr., Calderwood F W. Bull Alloy Phase Diagr, 1985; 6: 144 4 Donolato C, Steeb S. J Less-Common Met, 1969; 18: 442 5 McMasters O D, Gschneidner K A Jr., Venteicher R F. Acta Crystallogr, 1970; B26: 1224 6 Delfino S, Saccone A. Borsese A, Ferro R. Z Metallk, 1976; 67: 392 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|