| MOSSBAUER EFFECT STUDY OF YBa_2 Cu_(3-x)Sn_x o_(7-y) SYSTEM |
| WANG Genmiao;ZHANG Han;ZHANG Qirui;WU Yonghua Centre of Structure and Elements Analysis; University of Science and Technology of China; Hefei |
|
Cite this article:
WANG Genmiao;ZHANG Han;ZHANG Qirui;WU Yonghua Centre of Structure and Elements Analysis; University of Science and Technology of China; Hefei. MOSSBAUER EFFECT STUDY OF YBa_2 Cu_(3-x)Sn_x o_(7-y) SYSTEM. Acta Metall Sin, 1990, 26(5): 142-146.
|
|
|
Abstract Mossbauer spectra reveal that Sn exists in YBa_2Cu_(3-x)Snx O_(7-y) system(x=0.05, 0.10, 0.20, 0.30 and 0.40) in the form of Sn~(4+) and occupies Cu(Ⅰ) andCu(Ⅱ) sites. The relative rate at which Sn~(4+) occupies Cu(Ⅰ) or Cu(Ⅱ)sites varies with x. The superconductivity transition temperature, T_c, depressesa little due to the substitution of Cu for Sn.
|
|
Received: 18 May 1990
|
1 Gianpintzakis J, Matykiewicz J M, Kimball C W, Dwight A E, Dunlap B D, Slaski M, Fradin F Y. Phys Lett, 1987; A121: 307 2 Jayaram B, Agarwal S K, Gupta A, Narlikar A V. Jpn J Appl Phys,1987; 26: L1004 3 张酣,赵勇,周先意,王根苗,刘双怀,陈祖耀,夏健生,张其瑞.中国科学,待发表 4 Gonser U. Mossbauer Spectroscopy, Springer, 1975:39 5 Sharma R P, Prasad K G, Jayaram B, Agarwal S K. Gupta A, Narlikar A V. Phys Lett, 1988; A128: 127 6 Zhang Han. Wang Genmiao, Zhang Qirui. Phys Lett, 1989; A138: 517 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|