Please wait a minute...
Acta Metall Sin  1989, Vol. 25 Issue (5): 54-58    DOI:
Current Issue | Archive | Adv Search |
RECRYSTALLIZATION-INDUCED PLASTICITY PHENOMENON IN 18Ni MARAGING STEEL UNDER ELASTIC STRESS
YIN Zhongda;ZHOU Yongkang Harbin Institute of Technology Shanghai Centrifugal Machinery Research Institute YIN Zhongda; Pacxlty of Heat Treatment of Materials Harbin Institute of Technology; 150006 Harbin
Cite this article: 

YIN Zhongda;ZHOU Yongkang Harbin Institute of Technology Shanghai Centrifugal Machinery Research Institute YIN Zhongda; Pacxlty of Heat Treatment of Materials Harbin Institute of Technology; 150006 Harbin. RECRYSTALLIZATION-INDUCED PLASTICITY PHENOMENON IN 18Ni MARAGING STEEL UNDER ELASTIC STRESS. Acta Metall Sin, 1989, 25(5): 54-58.

Download:  PDF(1235KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The phenomenon of recrystallization-induced plasticity (RIP) in thecold-rolled (40-70% reduction) 18Ni maraging steel under elastic stress on heatingwas observed in research for the superplasticity during cyclic phase transformation.An approach to the RIP process has been made by the analysis of dynamic behav-iour of the alloy at elevated temperature, the phenomenological analysis of dynamicstrain feature curves, the confirmation of phase transformation point and TEM ob-servation of RIP processing itself.
Key words:  elastic stress      recrystallization      plasticity      maraging steel     
Received:  18 May 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I5/54

1 周永康.哈尔滨工业大学硕士学位论文,1988
2 胡郇.国外金属材料,1983;(1) :54
3 牧正志,田村今男.材料,1981;30(329) :211
4 Li J E M. J Appl Phys, 1962; 33: 2958
5 Bailey J E. Philos Mag, 1960; 5: 83
[1] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[2] XU Yongsheng, ZHANG Weigang, XU Lingchao, DAN Wenjiao. Simulation of Deformation Coordination and Hardening Behavior in Ferrite-Ferrite Grain Boundary[J]. 金属学报, 2023, 59(8): 1042-1050.
[3] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[4] LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling. Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy[J]. 金属学报, 2023, 59(7): 855-870.
[5] ZHANG Zhefeng, LI Keqiang, CAI Tuo, LI Peng, ZHANG Zhenjun, LIU Rui, YANG Jinbo, ZHANG Peng. Effects of Stacking Fault Energy on the Deformation Mechanisms and Mechanical Properties of Face-Centered Cubic Metals[J]. 金属学报, 2023, 59(4): 467-477.
[6] CHEN Xueshuang, HUANG Xingmin, LIU Junjie, LV Chao, ZHANG Juan. Microstructure Regulation and Strengthening Mechanisms of a Hot-Rolled & Intercritical Annealed Medium-Mn Steel Containing Mn-Segregation Band[J]. 金属学报, 2023, 59(11): 1448-1456.
[7] LOU Feng, LIU Ke, LIU Jinxue, DONG Hanwu, LI Shubo, DU Wenbo. Microstructures and Formability of the As-Rolled Mg- xZn-0.5Er Alloy Sheets at Room Temperature[J]. 金属学报, 2023, 59(11): 1439-1447.
[8] WU Caihong, FENG Di, ZANG Qianhao, FAN Shichun, ZHANG Hao, LEE Yunsoo. Microstructure Evolution and Recrystallization Behavior During Hot Deformation of Spray Formed AlSiCuMg Alloy[J]. 金属学报, 2022, 58(7): 932-942.
[9] ZHENG Shijian, YAN Zhe, KONG Xiangfei, ZHANG Ruifeng. Interface Modifications on Strength and Plasticity of Nanolayered Metallic Composites[J]. 金属学报, 2022, 58(6): 709-725.
[10] ZHANG Xinfang, XIANG Siqi, YI Kun, GUO Jingdong. Controlling the Residual Stress in Metallic Solids by Pulsed Electric Current[J]. 金属学报, 2022, 58(5): 581-598.
[11] GUO Xiangru, SHEN Junjie. Modelling of the Plastic Behavior of Cu Crystal with Twinning-Induced Softening and Strengthening Effects[J]. 金属学报, 2022, 58(3): 375-384.
[12] REN Shaofei, ZHANG Jianyang, ZHANG Xinfang, SUN Mingyue, XU Bin, CUI Chuanyong. Evolution of Interfacial Microstructure of Ni-Co Base Superalloy During Plastic Deformation Bonding and Its Bonding Mechanism[J]. 金属学报, 2022, 58(2): 129-140.
[13] JIANG Weining, WU Xiaolong, YANG Ping, GU Xinfu, XIE Qingge. Formation of Dynamic Recrystallization Zone and Characteristics of Shear Texture in Surface Layer of Hot-Rolled Silicon Steel[J]. 金属学报, 2022, 58(12): 1545-1556.
[14] GUO Haohan, YANG Jie, LIU Fang, LU Rongsheng. Constraint Related Fatigue Crack Initiation Life of GH4169 Superalloy[J]. 金属学报, 2022, 58(12): 1633-1644.
[15] HU Chen, PAN Shuai, HUANG Mingxin. Strong and Tough Heterogeneous TWIP Steel Fabricated by Warm Rolling[J]. 金属学报, 2022, 58(11): 1519-1526.
No Suggested Reading articles found!