| A NEW KIND OF QUENCHING INDUCED PLANAR DEFECT OF MARTENSITE IN Cu-Zn-Al ALLOY |
| ZHU Min;YANG Dazhi Dalian University of Technology |
|
Cite this article:
ZHU Min;YANG Dazhi Dalian University of Technology. A NEW KIND OF QUENCHING INDUCED PLANAR DEFECT OF MARTENSITE IN Cu-Zn-Al ALLOY. Acta Metall Sin, 1989, 25(2): 74-76.
|
|
|
Abstract A new kind of planar defect named non-basal plane stacking faults has been stud-ied using trace analysis and lattice image technique. It has been found that they are located in(125)_M plane of martensite lattice. By lattice image observation, the non-basal plane stackingfaults are argued to be induced by two incomplete basal plane stacking faults and may be theresults of fast quenching. The defects are regarded as anomalous structures of martensite.
|
|
Received: 18 February 1989
|
1 Otsuka K, Wayman C M. Scr Metall. 1975; 9: 1017 2 Adachi K, Perkins J. Metall Trans, 1985; 16A: 1551 3 Zhu Min (朱敏), Yang Dazhi (杨大智), Guo Kexin (Kuo K H) (郭可信). Chin J Met Sci Technol, 1987; 3: 194 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|