SNAP-ACTION PHASE TRANSFORMATION IN TWO-WAY SHAPE MEMORY Ni-Ti ALLOY |
LUO Laizhong;ZHANG Jinxiu;LIN Guangming Zhongshan University; Guangzhou |
|
Cite this article:
LUO Laizhong;ZHANG Jinxiu;LIN Guangming Zhongshan University; Guangzhou. SNAP-ACTION PHASE TRANSFORMATION IN TWO-WAY SHAPE MEMORY Ni-Ti ALLOY. Acta Metall Sin, 1989, 25(2): 77-78.
|
Abstract The snap-action behavior of a NiTi alloy disk which is controlled by combinationof a nonlinear stress field and temperature has been studied. After treatment for two-way shapememory, all shape memory strain of snap-action finishes abruptlyat certain temperature within aintertal of less than 1ms. The results of resistance measurement and in-situ X-ray diffractionindicate that, snap-action strain is mainly resulted from snap-action β→?R transformation.
|