MICROSTRUCTURES AND PROPERTIES OF SiC_w/Al COMPOSITES
GUO Shuqi;HAN Guihuan;YAO Zhongkai Harbin Institute of Technology
Cite this article: 

GUO Shuqi;HAN Guihuan;YAO Zhongkai Harbin Institute of Technology. MICROSTRUCTURES AND PROPERTIES OF SiC_w/Al COMPOSITES. Acta Metall Sin, 1988, 24(6): 499-504.

Download:  PDF(1895KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  This paper presents an investigation on the microstructures and prop-erties of the 17V.-% SiC_w/ZL109Al composites. TEM observations and EDAX ana-lysis revealed that aluminium diffuses into the SiC whiskers and that dislocationsexist at the whisker/matrix interfaces. Tensile test results showed that the isother-mal exposure and thermal cycle at both 573K and 733K caused the UTS reductionof the composites, the reduction in UTS due to thermal exposure at 733K beingmuch more significant than that due to thermal cycle at the same temperature.The SiC_w/ZL109Al composites were also found to have exellent wear resistance,which does not seem to vary much with the volume content of whiskers in therange of 11--17%.
Key words:  composites      SiC whisker      microstructure      strength     
Received:  18 June 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I6/499

1 McDanels D L, Hoffman C A. NASA-TM-83610, 1982
2 Starke E A Jr., Sanders T H Jr., Palmer I G. J Met, 1981; 33: 24
3 Divecha A P, Fishman S G. In: Miller K J, Smith R F eds., Machanical Behavior of Materials, Vol. Ⅲ, Proc 3rd Int Conf on Machanical Behavior of Materials, Cambridge, Aug, 20--24, 1979, Oxford: Pergamon, 1980: 351
4 Nieh T G, Rainen R A, Chellman D J, In: Harrigan W C Jr., Strife J, Dhingra A K eds., Proc 5th Int Conf on Composites Materials, ICCM/2, San Diego Califonia, USA, 29--30 July, 1 Aug., 1985, Warrendale: Metallutgical Society of AIME, 1985: 825
5 Sakamoto A, Hasegawa H, Minoda Y. In: Harrigan W C Jr., Strife J, Dhingra A K. eds. Proc 5th Int Conf on Composites Materials, ICCM/2, San Diego Califonia, USA, 29--30 July. 1 Aug., 1985, Warrendale: Metallutgical Society of AIME, 1985: 699
6 Phillips W L. Proc of the 1978 Int Conf on Composites Materials ICCM/2, Toronto, Canada, Apr. 16--20, 1978, Warrendale: Metallutgical Society of AIME, 1978: 567
7 Parrat N J. Fiber Reinforced Materials Technology, London, U. K.: Van Nostrand-Reinhold, 1972: 159
8 郭树启,曹利,韩圭焕,姚忠凯.复合材料学报,1987;4(3) :32
9 Nutt S R. J Am Ceram Soc, 1984; 67 (6) : 428
10 堂,本忠,立松义明,田中淳夫.日本公开特许.昭59-70736,1984:179%
[1] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[2] FENG Qiang, LU Song, LI Wendao, ZHANG Xiaorui, LI Longfei, ZOU Min, ZHUANG Xiaoli. Recent Progress in Alloy Design and Creep Mechanism of γ'-Strengthened Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1125-1143.
[3] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[4] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[5] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[6] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[7] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[8] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[9] LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling. Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy[J]. 金属学报, 2023, 59(7): 855-870.
[10] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[11] WANG Zongpu, WANG Weiguo, Rohrer Gregory S, CHEN Song, HONG Lihua, LIN Yan, FENG Xiaozheng, REN Shuai, ZHOU Bangxin. {111}/{111} Near Singular Boundaries in an Al-Zn-Mg-Cu Alloy Recrystallized After Rolling at Different Temperatures[J]. 金属学报, 2023, 59(7): 947-960.
[12] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[13] LIANG Kai, YAO Zhihao, XIE Xishan, YAO Kaijun, DONG Jianxin. Correlation Between Microstructure and Properties of New Heat-Resistant Alloy SP2215[J]. 金属学报, 2023, 59(6): 797-811.
[14] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[15] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
No Suggested Reading articles found!