INFLUENCE OF PROCESS PARAMETERS ON THE PERFORMANCE UNIFORMITY OF DETONATION GUN SPRAYED WC-Co COATINGS |
WANG Tiegang1), SONG Binghong2), HUA Weigang1), GONG Jun1), SUN Chao1) |
1) State Key Laboratory of Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
2) AVIC Harbin Dong'an Engine (Group) Co., Ltd., Harbin 150066 |
|
Cite this article:
WANG Tiegang SONG Binghong HUA Weigang GONG Jun SUN Chao. INFLUENCE OF PROCESS PARAMETERS ON THE PERFORMANCE UNIFORMITY OF DETONATION GUN SPRAYED WC-Co COATINGS. Acta Metall Sin, 2011, 47(1): 115-122.
|
Abstract Based on the orthogonal experiment, the effects of oxygen-fuel ratio and spraying distance on physical and mechanical properties of D-gun sprayed WC-Co coatings were investigated. An ideal coating with the uniform dense microstructures, high hardness and elastic modulus, and excellent wear resistance was obtained by technology optimization. The phase identifications and microstructure observation of the optimized WC-Co coating were conducted by XRD and SEM, respectively. The coating showed near-isotropic behaviors, which has been verified by the comparisons of mechanical and wear properties between cross section and surface. The mechanisms how the spraying parameters affected near--isotropic characters of the D-gun sprayed WC-Co coating were analyzed and discussed.
|
Received: 14 July 2010
|
|
[1] Lima R S, Karthikeyan J, Kay C M, Lindemann J, Berndt C C. Thin Solid Films, 2002; 416: 129[2] Picas J A, Xiong Y, Punset M, Ajdelsztajn L, Forn A, Schoenung J M. Int J Refract Met Hard Mater, 2009; 27: 344[3] Kucuk A, Lima R S, Berndt C C. J Am Ceram Soc, 2001; 84: 685[4] Kulkarni A, Vaidya A, Goland A, Sampath S, Herman H. Mater Sci Eng, 2003; A359: 100[5] Nakamura T, Qian G, Berndt C C. J AmCeramSoc, 2000; 83: 578[6] Friis M, Persson C, Wigren J. Surf Coat Technol, 2001; 141: 115[7] Gahlin R, Larsson M, Hedenqvist P, Jacobson S, Hogmark S. Surf Coat Technol, 1997; 90: 107[8] Archard J F. J Appl Phys, 1953; 24: 981[9] Kassman A, Jacobson S, Erickson L, Hedenqvist P, Olsson M. Surf Coat Technol, 1991; 50: 75[10] Bemporad E, Sebastiani M, Felicis D D, Carassiti F, Valle R, Casadei F. Thin Solid Films, 2006; 515: 186[11] Trezona R I, Hutchings I M. Wear, 1999; 233–235: 209[12] Shipway P H, Hutchings I M. Surf Coat Technol, 1995; 71: 1[13] Gee M G, Gant A, Hutchings I M, Bethke R, Schiffman K, Acker K V, Poulat S, Gachon Y, Stebut J V. Wear, 2003; 255: 1[14] Kusano Y, Acker K V, Hutchings I M. Surf Coat Technol, 2004; 183: 312[15] Du H, Hua W G, Liu J G, Gong J, Sun C, Wen L S. Mater Sci Eng, 2005; A408: 202[16] Lima R S, Marple B R. Acta Mater, 2004; 52: 1163[17] Mcpherson R. Thin Solid Films, 1981; 83: 297[18] Yang J F, Ohji T, Kanzaki S, Diaz A, Hampshire S. J Am Ceram Soc, 2002; 85: 1512[19] Bolelli G, Cannillo V, Lusvarghi L, Manfredini T, Siligardi C, Bartuli C, LoretoA, Valente T. J Eur CeramSoc, 2005; 25: 1835[20] Camerucci M A, Urretavizcaya G, Cavalieri A L. J Eur Ceram Soc, 2001; 21: 1195[21] Mellali M, Fauchais P, Grimaud A. Surf Coat Technol, 1996; 81: 275[22] Ban Z G, Shaw L L. Acta Mater, 2001; 49: 2933[23] Fervel V, Normand B, Liao H, Coddet C, Beche E, Berjoan R. Surf Coat Technol, 1999; 111: 255[24] Semenov S Y, Cetegen B M. Mater Sci Eng, 2002; A335: 67[25] Wang T G, Zhao S S, Hua W G, Gong J, Sun C. Surf Coat Technol, 2009; 203: 1637[26] Cartier M, McDonnell L, Cashell E M. Surf Coat Technol, 1991; 48: 241[27] Matejicek J, Sampath S, Brand P C, Prask H J. Acta Mater, 1999; 47: 607[28] Allen A J, Ilavsky J, Long G G, Wallace J S, Berndt C C, Herman H. Acta Mater, 2001; 49: 1661[29] Kroupa F, Dubsky J. Scr Mater, 1999; 40: 1249[30] Jin G, Xu B S, Wang H D, Li Q F,Wei S C. Mater Lett, 2007; 61: 2454 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|