WANG Xing, XI Wenjun, CUI Yue, LI Shujie. MICROSTRUCTURE EVOLUTION MECHANISM AND MECHANICAL PROPERTIES OF FeNiCrAl ALLOY REINFORCED BY COHERENT NiAl SYNTHE- SIZED BY THERMITE PROCESS. Acta Metall Sin, 2015, 51(4): 483-491.
The excellent thermal conductivity, low thermal expansion and high oxidation resistance of ferritic FeNiCrAl alloys, provide them with the potential to be replacements for nickel-based superalloys in high-temperature applications. However, their usage is limited, because of their poor high-temperature mechanical properties. The high melting point of NiAl intermetallic compounds, together with their excellent high temperature stability and similar lattice parameters to a-Fe, allow them to be used to coherently strengthen ferritic FeNiCrAl alloys to extend their high-temperature performance. Traditionally, these Fe(Ni, Cr)/NiAl alloys are prepared by vacuum reaction melting followed by an aging process. But the aging process has drawbacks including excessive cost, the length of aging time required and coarsening of the NiAl phase at high temperature. A more cost-effective thermite reaction process, was tried to prepare the Fe(Ni, Cr)/NiAl alloys. In this route, ferrite FeNiCrAl alloys were strengthened by a high volume fraction nanoscale-NiAl phase which was achieved without using the aging process. Several types of thermites were designed and studies were conducted to explore the transformations of the alloy microstructures and the changes of the tensile properties with the various thermite compositions. The microstructures of these thermites synthesized Fe(Ni, Cr)/NiAl alloys were investigated using XRD, SEM, EDS, TEM and SAED. The effect of Al content in the thermites on the microstructures of the alloys was studied. Experimental results showed that when the thermites contained no more than 25.4% (mass fraction) of Al, the synthesized Fe(Ni, Cr)/NiAl alloys were composed primarily of an austenite phase. The main component phase of the alloy composites was transformed into ferrite when the mass fraction of Al in the thermites was 26.6%, meanwhile the NiAl particle precipitates arose. As the Al content of the mixture was further increased, the NiAl precipitates were gradually replaced by an intertexture structure. The intertexture structure was totally dominant when the mass fraction of Al in the thermites was 31.4%. Experimental results showed that this intertexture microstructure material was composed of a ferritic FeNiCrAl matrix with a width of 80~100 nm and NiAl precipitates with a width of about 50 nm, and the two phases matched coherently. This microstructure resulted from liquid spinodal decomposition. The effect of Al content on the mechanical properties of the alloys was also investigated. The increase of the Al content in the thermites resulted in a decrease of the elongation of the alloys, which varied from 25.5% to 1.7% when the mass fraction of Al ranged from 24.2% to 29.0%. When the thermites contained 26.6% mass fraction of Al, the tensile strength of the alloy achieved its maximum value of 640.87 MPa.
Table 1 Chemical composition and content of thermites
Fig.2 SEM images of Fe(Ni, Cr)/NiAl alloys with Al contents of 24.2% (a), 25.4% (b), 26.6% (c), 27.8% (d, e), 29.0% (f), 30.2% (g) and 31.4% (h, i) in thermites
Fig.3 XRD spectra of Fe(Ni, Cr)/NiAl alloys with different Al contents in thermites
Composition
Fe
Ni
Cr
Al
Atomic fraction / %
54.30
20.78
23.64
1.28
Mass fraction / %
54.97
22.11
22.29
0.63
Table 2 EDS results of the alloy with Al content of 24.2% in thermites
Composition
Fe
Ni
Cr
Al
Atomic fraction / %
50.67
21.75
26.11
1.47
Mass fraction / %
51.41
23.20
24.67
0.72
Table 3 EDS results of the alloy with Al content of 26.6% in thermites
Fig.4 TEM images of the square microstructure (a), intertexture microstructure (b) and transition region of the square microstructure and the intertexture microstructure (c) (Insets show the corresponding SAED patterns)
Fig.5 SEM images of Fe(Ni, Cr)/NiAl alloys with Al content of 31.4% in thermites without aging (a) and aged at 500 ℃ (b), 700 ℃ (c) and 900 ℃ (d) for 100 min
Fig.6 Tensile stress-strain curves of Fe(Ni, Cr)/NiAl alloys with different Al contents in thermites
Fig.7 Effect of Al content in thermites on tensile strength and elongation of Fe(Ni, Cr)/NiAl alloys
Fig.8 SEM images of the fracture morphologies of Fe(Ni, Cr)/NiAl alloys with Al contents of 24.2% (a, b), 26.6% (c, d) and 29.0% (e, f) in thermites
[1]
Masuyama F. ISIJ Int, 2001; 41: 612
[2]
Calderon H, Fine M E. Mater Sci Eng, 1984; 63: 197
[3]
Pearson W B. A Handbook of Lattice Spacings and Structures of Metals and Alloys. Oxford: Pergamon Press, 1958: 347
[4]
Stallybrass C, Schneider A, Sauthoff G. Intermetallics, 2005; 13: 1263
[5]
Sudbrack C K, Yoon K E, Noebe R D, Seidman D N. Acta Mater, 2006; 54: 3199
[6]
Calderon H A, Fine M E, Weertman J R. Metall Trans, 1988; 19A: 1135
[7]
Hao S M, Ishida K, Nishizawa T. Metall Trans, 1985; 16A: 179
[8]
Stallybrass C, Sauthoff G. Mater Sci Eng, 2004; A387: 985
[9]
Vo N Q, Liebscher C H, Rawlings M J, Asta M, Dunand D C. Acta Mater, 2014; 71: 89
[10]
Bradley A J, Taylor A. Proc R Soc London, 1938; 166(A926): 353
[11]
Yin S. Combustion Synthesis. Beijing: Metallurgical Industry Press, 2004: 1
(殷 声. 燃烧合成. 北京: 冶金工业出版社, 2004: 1)
[12]
Borovinskaya I P. Pure Appl Chem, 1992; 64: 919
[13]
Yukhvid V I. Pure Appl Chem, 1992; 64: 977
[14]
Fu Z Y. Acta Mater Comp Sin, 2000; 17(1): 5
(傅正义. 复合材料学报, 2000; 17(1): 5)
[15]
Hao S M, Takayama T, Ishida K, Nishizawa T. Metall Trans, 1984; 15A: 1819
[16]
Bradley A J. J Iron Steel Inst, 1949; 163: 19
[17]
Bradley A J. J Iron Steel Inst, 1951; 168: 233
[18]
Bradley A J. J Iron Steel Inst, 1952; 171: 41
[19]
Hanna J A, Baker I, Wittmann M W, Munroe P R. J Mater Res, 2005; 20: 791
[20]
Cahn J W. Acta Metall, 1961; 9: 795
[21]
Cahn J W. Acta Metall, 1962; 10: 179
[22]
Cahn J W. Acta Metall, 1962; 10: 907
[23]
Xi W, Peng R L, Wu W, Li N, Wang S, Johansson S. J Mater Sci, 2012; 47: 3585
[24]
Zhang C Q, Yao K F. Acta Metall Sin, 2006; 42: 870
(张长青, 姚可夫. 金属学报, 2006; 42: 870)
[25]
Ma N G, Kui H W. China Mech Eng, 2000; 11: 1298
(马南钢, Kui H W. 中国机械工程, 2000; 11: 1298)
[26]
Lee K L, Kui H W. J Mater Res, 1999; 14: 3653
[27]
Yuen C W, Lee K L, Kui H W. J Mater Res, 1997; 12: 314
[28]
Taillard R, Pineau A, Thomas B J. Mater Sci Eng, 1982; 54: 209
[29]
Rothman M F. High-Temperature Property Data: Ferrous Alloys. Metals Park, OH: ASM International, 1987: 250
[30]
Teng Z K, Liu C T, Ghosh G, Liaw P K, Fine M E. Intermetallics, 2010; 18: 1437