关于Fe-28Al合金中的析出相 |
赵钟涛;刘涛;马如璋;马长英 |
北京科技大学;冶金工业部钢铁研究总院 |
|
ON THE PRECIPITATE IN Fe-28Al ALLOY |
ZHAO Zhongtao; LIU Tao; MA Ruzhang (University of Scicnce and Technology Beijing; Beijing 100083); MA Changying (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing 100081 ) |
引用本文:
赵钟涛;刘涛;马如璋;马长英. 关于Fe-28Al合金中的析出相[J]. 金属学报, 1996, 32(6): 585-588.
,
,
,
.
ON THE PRECIPITATE IN Fe-28Al ALLOY[J]. Acta Metall Sin, 1996, 32(6): 585-588.
1MckameyCG,HortonJA,LiuCT.JMaterRes,1989;4:11562DuG,WangZ,XiaoJ.ScrMetallMater,1994;30:15593杜国维,王政,肖纪美.金属学报,1995;31:A1514中宪典,山村明彦,羽坂雅之,江口铁男.日本金属学会志,1977;41:2935OkamotoH,BeckPA,MetallTrans,1971;2.5696MorgandP,MetallTrans,1970:1:23317MorralFR.JIronSteelInstLondon,1934;130:4198BB.MuTOM,1962;(6):29KerrWR.MetallTrans,1986;17A:229810SnoekJL.NewDevelopmentsinFerromagneticMaterials.Moscow:Foreignliteraturepress,1949:110(inRussian) |
|