抽拉速率跃迁对定向凝固单晶高温合金DD3一次枝晶间距和微观偏析的影响 |
黄太文;刘林;张卫国;张军;傅恒志 |
西北工业大学凝固技术国家重点实验室; 西安710072 |
|
INFLUENCE OF WITHDRAWING RATE TRANSITION ON THE PRIMARY DENDRITE ARM SPACING AND MICROSEGREGATION OF DIRECTIONALLY SOLIDIFIED SINGLE CRYSTAL SUPERALLOY DD3 |
HUANG Taiwen; LIU Lin; ZHANG Weiguo; ZHANG Jun; FU Hengzhi |
State Key Laboratory of Solidification Processing; Northwestern Polytechnical University; Xi'an 710072 |
引用本文:
黄太文 刘林 张卫国 张军 傅恒志. 抽拉速率跃迁对定向凝固单晶高温合金DD3一次枝晶间距和微观偏析的影响[J]. 金属学报, 2009, 45(10): 1225-1231.
,
,
,
,
.
INFLUENCE OF WITHDRAWING RATE TRANSITION ON THE PRIMARY DENDRITE ARM SPACING AND MICROSEGREGATION OF DIRECTIONALLY SOLIDIFIED SINGLE CRYSTAL SUPERALLOY DD3[J]. Acta Metall Sin, 2009, 45(10): 1225-1231.
[1] Li S M, Du W, Zhang J, Li J S, Liu L, Fu H Z. Acta Metall Sin, 2002; 38: 1195
(李双明, 杜炜, 张军, 李金山, 刘 林, 傅恒志. 金属学报, 2002; 38: 1195)
[2] Ma D X. Metall Trans, 2004; 35B: 741
[3] Elliott A J. PhD Thesis, Michigan University, Michigan, 2005
[4] Smith V G, Tiller W A, Rutter J W. Can J Phys, 1955; 33: 723
[5] Li S M, Fu H Z. Sci China, 2008; 38E: 402
(李双明, 傅恒志. 中国科学, 2008; 38E: 402)
[6] Warren J A, Langer J S. Phy Rev, 1993; 47E: 2702
[7] Wang W, Lee P D, McLean M. Acta Mater, 2003; 51: 2971
[8] Ding G L, Huang W D, Zhou Y. J Mater Sci Lett, 1997; 16: 376
[9] Hui J, Tiwari R, Wu X, Tewari S N, Trivedi R. Metall Trans, 2002; 33A: 3499
[10] Guo Y G, Li S M, Liu L, Fu H Z. Acta Metall Sin, 2008; 44: 365
(郭勇冠, 李双明, 刘林, 傅恒志. 金属学报, 2008; 44: 365)
[11] Hunt J D. Solidification and Casting of Metals. The Metals Society, London, 1979: 3
[12] Kurz W, Fisher D J. Acta Mater, 1981; 29: 11
[13] Ma D X, Sahm P R. Metall Trans, 1998; 29A: 1113
[14] Hut J D, Lu S Z. Metall Trans, 1996; 27A: 611
[15] Li L C. PhD Thesis, Auburn University, Alabama, 2002
[16] Ma D X, Sahm P R. Metall Trans, 1992; 23A: 3377
[17] Karunaratne M S A, Rae C M F, Reed R C. Metall Trans, 2001; 32A: 2001
[18] Zimmermann G, Weiss A. Microgravity Sci & Tech, 2005; 16: 141
[19] Zou M M, Zhang J, Liu L, Fu H Z. Acta Metall Sin, 2008; 44: 150
(邹敏明, 张军, 刘林, 傅恒志. 金属学报, 2008; 44: 150)
[20] Warren J A, Langer J S. Phy Rev, 1990; 42A: 3518
[21] Basaran M. Metall Trans, 1981; 12A: 1235 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|