| 两种电弧离子镀Ni-Co-Cr-Al-Si-Y涂层的高温氧化行为 |
| 徐朝政;姜肃猛;马军;宫骏;孙超 |
| 中国科学院金属研究所金属腐蚀与防护国家重点实验室; 沈阳 110016 |
|
| HIGH TEMPERATURE OXIDATION BEHAVIOR OF TWO NiCoCrAlSiY COATINGS DEPOSITED BY ARC ION PALTING |
| XU Chaozheng; JIANG Sumeng; MA Jun; GONG Jun; SUN Chao |
| State Key Laboratory for Corrosion and Protection; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
徐朝政 姜肃猛 马军 宫骏 孙超. 两种电弧离子镀Ni-Co-Cr-Al-Si-Y涂层的高温氧化行为[J]. 金属学报, 2009, 45(8): 964-970.
,
,
,
,
.
HIGH TEMPERATURE OXIDATION BEHAVIOR OF TWO NiCoCrAlSiY COATINGS DEPOSITED BY ARC ION PALTING[J]. Acta Metall Sin, 2009, 45(8): 964-970.
| [1] Jeanine T D, Dinesh K G. Surf Coat Technol, 1994; 68–69:1
[2] Goward G W. Surf Coat Technol, 1998; 108–109: 73
[3] Nicholls J R. Mater Res Bull, 2003; 28: 1
[4] Brandl W, Grabke H J, Toma D, Kruger J. Surf Coat Technol, 1996; 86–87: 41
[5] Wu Y N, Qin M, Feng Z C, Liang Y, Sun C, Wang F H. Mater Lett, 2003; 57: 2404
[6] Tang F, Ajdelsztajn L, Schoenung J M. Oxid Met, 2004; 61: 219
[7] Wang B, Gong J, Sun C, Huang R F, Wen L S. Mater Sci Eng, 2003; A357: 39
[8] Guo M H, Wang Q M, Ke P L, Gong J, Sun C, Huang R F, Wen L S. Surf Coat Technol, 2006; 200: 3942
[9] Smeggil J G. Mater Sci Eng, 1987; A87: 261
[10] Sun C, Wang Q M, Tang Y J, Guan Q F, Gong J, Wen L S. Acta Metall Sin, 2005; 41: 1167
(孙 超, 王启民, 唐永吉, 关庆丰, 宫 骏, 闻立时. 金属学报, 2005; 41: 1167)
[11] Tolpygo V K, Clarke D R. Acta Mater, 1999; 47: 3589
[12] Dryepondt S, Clarke D R. Scr Mater, 2009; 60: 917
[13] Prescott R, Graham M J. Oxid Met, 1992; 38: 233
[14] Li M S. High Temperature Corrosion of Metals. Beijing:Metallurgical Industry Press, 2001: 37
(李美栓. 金属的高温腐蚀. 北京: 冶金工艺出版社, 2001: 37)
[15] Itoh Y, Saitoh M, Ishiwata Y. J Mater Sci, 1999; 34: 3957
[16] Knotek O, L¨offler F, Beele W. Surf Coat Technol, 1993;61: 6
[17] Lou H Y, Wang F H. Vacuum, 1992; 43: 757
[18] Wang Q M, Zhang K, Gong J, Cui Y Y, Sun C, Wen L S. Acta Mater, 2007; 55: 1427
[19] Maxim K, David H P, Christoph T, Hans–Peter B, Christoph S. US Pat, US6 383 312, 2002
[20] Sakata M, Hayashi S, Nishimoto T, Yoshioka T, Narita T. Oxid Met, 2007; 68: 295
[21] Sumoyama D, Thosin K Z, Nishimoto T, Yoshioka T, Izumi T, Hayashi S, Narita T. Oxid Met, 2007; 68: 313 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|