| 纯Mg的蠕变行为研究 |
| 晏井利;孙扬善;薛烽;陶卫建 |
| 东南大学江苏省先进金属材料高技术研究重点实验室 |
|
| An investigation on the creep behavior of pure magnesium |
| ;;; |
| 东南大学材料科学与工程学院 |
引用本文:
晏井利; 孙扬善; 薛烽; 陶卫建 . 纯Mg的蠕变行为研究[J]. 金属学报, 2008, 44(11): 1354-1359 .
,
,
,
.
An investigation on the creep behavior of pure magnesium[J]. Acta Metall Sin, 2008, 44(11): 1354-1359 .
[1]Luo A A.Int Mater Rev,2004;49:13 [2]Wang Q D,Zeng X Q,L(?) Y Z,Ding W J.Mater Rev, 2000;14(3):21 (王渠东,曾小勤,吕宜振,丁文江.材料导报,2000;14(3):21) [3]Wang X Q,Li Q A,Zhang X Y.Light Metals,2007;6:45 (王小强,李全安,张兴渊.轻金属,2007;6:45) [4]Zhang J,Pan F S,Li Z S.Foundry,2004;53:770 (张静,潘复生,李忠盛.铸造,2004;53:770) [5]Mordike B L.Mater Sci Eng,2002;A324:103 [6]Pekguleryuz M O,Kaya A A.Adv Eng Mater,2003;12: 866 [7]Zhang X M,Peng Z K,Chen J M,Deng Y L.Chin J Nonferr Metals,2004;14:1443 (张新明,彭卓凯,陈健美,邓运来.中国有色金属学报,2004;14:1443) [8]Shi L,Northwood D O.Acta Metall Mater,1994;42:871 [9]Jones R B,Harris J E.Joint Int Conf Creep,Part 3A, London:The Institution of Mechanical Engineers,1963:1 [10]Vagarali S S,Langdon T G.Acta Metall,1981;29:1969 [11]Roberts S.Trans Am Inst Min Metall Eng,1953;197:732 [12]Mili(?)ka K,(?)adek J,Ry(?) P.Acta Metall,1970;18:1071 [13]Kim W J,Chung S W,Chung C S,Kum D.Acta Mater, 2001;49:3337 [14]Chung S W,Watanabe H,Kim W J,Higashi K.Mater Trans JIM,2004;45:1266 [15]Kassner M E,Pérez-Prado M T.Fundamentals of Creep in Metals and Alloys.Oxford:Elsevier Ltd.,2004:1 [16]Sherby O D,Burke P M.Prog Mater Sci,1968;13:323 [17]Sherby O D,Weertman J.Acta Metall,1979;27:387 [18]Poirier J P.Acta Metall,1978;26:629 [19]Nabarro F R N.Mater Sci Eng,2004;A387-389:659 [20]Nabarro F R N.Acta Mater,2006;54:263 [21]Tegart W J.Acta Metall,1961;9:614 [22]Northwood D O,Daly K E,Smith I O.Mater Sci Eng, 1985;72:51 [23]Langdon T G.Philos Mag,1970;22(178):689 [24]Langdon T G.J Mater Sci,2006;41:597 [25]Bell R L,Langdon T G.J Mater Sci,1967;2:313 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|