| 连铸结晶器内簇状夹杂物分形生长的Monte--Carlo模拟 |
| 雷洪;赫冀成 |
| 东北大学材料电磁过程研究教育部重点实验室 |
|
| Monte-Carlo Simulation for Fractal Growth of inclusions in the Continuous Casting Mold |
| ;Jicheng He |
| 东北大学材料电磁过程研究教育部重点实验室 |
引用本文:
雷洪; 赫冀成 . 连铸结晶器内簇状夹杂物分形生长的Monte--Carlo模拟[J]. 金属学报, 2008, 44(6): 698-702 .
,
.
Monte-Carlo Simulation for Fractal Growth of inclusions in the Continuous Casting Mold[J]. Acta Metall Sin, 2008, 44(6): 698-702 .
[1]Zhang L.Steel Res lnt,2005;76:784 [2]Lei H,Zhu M Y,He J C.J Iron Steel Res lnt,2003:10(2): 21 [3]Aboutalebi M R,Hasan M,Guthrie R I L.Metall Mater Trans,1995;26B:731 [4]Miki Y,Shimada Y,Thomas B G,Denissov A.Iron Steel- maker,1997;24(8):31 [5]Zhang B W,Deng K,Lci Z S,Ren Z M.Acta Metall Sin, 2004;40:623 (张邦文,邓康,雷作胜,任忠鸣.金属学报,2004:40:623) [6]Zhang L,Taniguchi S,Cai K.Metall Mater Trans,2000; 31B:253 [7]Nakanishi K,Szekely J.Trans ISIJ,1975;15:522 [8]Javurek M,Gittlcr P,Rossler R,Kaufmann B,Prcblinger H.Steel Res lnt,2005;76:64 [9]Sinha A K,Sahai Y.ISIJ lnt,1993;33:556 [10]Wang L T,Peng S H,Zhang Q Y,Li Z B.Steel Res Int, 2006;77:25 [11]Zhao L G,Liu K.J Res Iron Steel,2002:14(6):19 (赵连刚,刘坤.钢铁研究学报,2002;14(6):19) [12]Lei H,Wang L,Wu Z,Fan J.ISIJ lnt,2002;42:717 [13]Launder B E,Spalding D B.Comput Meth Appl Meeh En9,1974;15:269 [14]O′Rourke P J.PhD Thesis,Princeton University,New.Jer- sey,USA,1981 [15]Taniguchi S,Kikuchi A,Ise T,Shoji N.ISIJ Int.1996;36 (Suppl.):117 [16]Thomas B G,Mika L J,Najjar F M.Metall Trans,1990; 21B:387 [17]Thomas B G,Huang X,Sussman R C.Metall Mater Trans,1994;25B:527 [18]Bouris D,Bergeles G.Metall Mater Trans,1998;29B:641 [19]Lei H,Jin Y,Zhu M,He J.J Mater Sei Technol,2002;18: 403 [20]Lu L F,Lu S P,Zhou S Q,Ren Q,Li D,Kang R M,Wu W D.J Chongqing Univ,2006;29(2):72 (刘林飞,刘守平,周土祺,任勤,李丁,康人木,吴文东.重庆大学学报,2006;29(2):72) [21]Yin H,Shibata H,Emi T,Suzuki M.ISIJ lnt,1997;37: 936 [22]Kimura S,Nabeshima Y,Nakajima K,Mizoguchi S.Metall Mater Trans,2000;31B:1013 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |