					引用本文:
						|  |  
    					|  |  
    					| 高压条件下Pd--Ni合金熔体非晶形成过程及微观结构演化的分子动力学研究 |  
						| 戚  力  董立峰  程  华  崔占全  马明臻   景  勤  李  工 |  
					| 燕山大学亚稳材料制备技术与科学国家重点实验室; 秦皇岛 066004 |  
						|  |  
    					| Glass formation and local structure evolution in rapid cooled Pd-Ni alloy melts under high pressure |  
						| ;;;;Zhuang-Qi HU; |  
						| 燕山大学;亚稳材料制备技术与科学国家重点实验室 |  
								戚力; 董立峰; 程华; 崔占全; 马明臻; 景勤 ; 李工                                                                                                                                                                                                                      . 高压条件下Pd--Ni合金熔体非晶形成过程及微观结构演化的分子动力学研究[J]. 金属学报, 2008, 44(2): 233-236       .	
																												,
																								 ,
																								 ,
																								 ,
																								 ,
																								 ,
																												 . 
				Glass formation and local structure evolution in rapid cooled Pd-Ni alloy melts under high pressure[J]. Acta Metall Sin, 2008, 44(2): 233-236       .
 
					
						| 
								
									|  
          
          
            
                         
            
									            
									                
																														  
																| [1]Li M,Johnson W L.Phys Rev Left,1993;70:1120 [2]Inoue A.Acta Mater,2000;48:279
 [3]Johnson W L.MRS Bull,1999;24:42
 [4]Johnson W L.Mater Sci Forum,1996;35:225
 [5]Wang D,Li Y,Sun B B,Sui M L,Lu K,Ma E.Appl Phys Lett,2004;84:4029
 [6]Tang M B,Zhao D Q,Pan M X,Wang W H.Chin Phys Lett,2004;21:901
 [7]Duan G,Xu D,Zhang Q,Zhang G,Cagin T,Johnson W L,Goddard W A.Phys Rev,2005;71B:223208
 [8]Xia L,Li W H,Fang S S,Wei B C,Dong Y D,J Appl Phys,2000;699:026103; Yao K F,Ruan F.Chin Phys Lett,2005;22:1481; Yao K F,Ruan F,Yang Y Q,Chen N.Appl Phys Lett, 2006;88:122106
 [9]Zhang J Z,Zhao Y S.Nature,2004;430:332
 [10]Zhang J Z,Zhao Y S.Nature,2005;437:1057
 [11]Wang Y,Fang Y Z,Kikegawa T,Lathe C,Saksl K,Franz H,Schneider J R,Genward L,Wu F M,Liu J F,Jiang J Z.Phys Rev Lett,2005;95:155501
 [12]Steinhardt P J,Nelson D R,Ronchetti M.Phys Rev,1993; 28B:784
 [13]Nakano H,Qi D W,Wang S.J Chem Phys,1989;90:1871
 [14]Qi D W,Wang S.J Non-Cryst Solid,1991;13:573
 [15]Coluzzi B,Parisi G,Verrocchio P.Phys Rev Lett,2000; 84:306
 [16]Morishita T.Phys Rev Lett,2006;97:165502
 [17]Li H,Pederiva F.Phys Rev,2005;71B:054513
 [18]Shen Z Y,Chen G Y,Zhang Y,Yin X J.Phys Rev,1989; 39B:2714
 [19]Wang W K,Iwasaki H,Fukamichi K.J Mater Sci,1980; 15:2701
 [20]K(?)ga J,Okumura H,Nishio K,Yamaguchi T,Yonezawa F.Phys Rev,2002;66B:064211
 [21]Wang W H,Okada T,Wen P,Wang X L,Pan M X,Zhao D Q,Utsumi W.Phys Rev,2003;68B:184105
 [22]Fraenkel W,Stern A.Z Anorg Chem,1927;166:161
 [23]Foiles S M.Phys Rev,1985;32B:3409
 [24]Lu J,Szpunar J A.Philos Mag,1997;75:1057
 [25]Verlet V.Phys Rev,1967;159:98
 [26]Andersen H C.J Chem Phys,1980;72:4
 [27]Weaire D.J Phys,1968;C1:210
 [28]Honeycutt J D,Andersen H C.J Phys Chem,1987;91: 4950
 [29]Qi L,Zhang H F,Hu Z Q,Liaw P K.Phys Lett,2004; 327A:506
 [30]Rahman A,Mandell M J,McTague J P.J Chem Phys, 1976;64:3215
 |  
             
												
											    	
											        	|  | Viewed |  
											        	|  |  |  
												        |  | Full text 
 | 
 
 |  
												        |  |  |  
												        |  | Abstract 
 | 
 |  
												        |  |  |  
												        |  | Cited |  |  
												        |  |  |  |  
													    |  | Shared |  |  
													    |  |  |  |  
													    |  | Discussed |  |  |  |  |