| 接触模型对搅拌摩擦焊接数值模拟的影响 |
| 张昭;张洪武 |
| 大连理工大学工程力学系 |
|
| EFFECT OF CONTACT MODEL ON NUMERICAL SIMULATION OF FRICTION STIR WELDING |
| 大连理工大学工程力学系 |
引用本文:
张昭; 张洪武 . 接触模型对搅拌摩擦焊接数值模拟的影响[J]. 金属学报, 2008, 44(1): 85-90 .
[1]Mishra R S,Ma Z Y.Mater Sci Eng,2005;R50:1 [2]Ericsson M,Sandstr(?)m R.Int J Fatigue,2003;25:1379 [3]Peel M,Steuwer A,Preuss M,Withers P J.Acta Mater, 2003;51:4791 [4]Gharacheh M A,Kokabi A H,Daneshi G H,Shalchi B, Sarrafi R.Int J Mach Tools Manuf,2006;46:1983 [5]James M N,Hattingh D G,Bradley G R.Int J Fatigue, 2003;25,1389 [6]Kim Y G,Fujii H,Tsumura T,Komazaki T,Nakata K. Mater Lett,2006;60:3830 [7]Hassan Kh A A,Prangness P B,Norman A F,Price D A, Williams S W.Sci Technol Weld Joining,2003;8:257 [8]Attallah M M,Salem H G.Mater Sci Eng,2005;A391: 51 [9]Reynolds A P,Tang W,Khandkar Z,Khan J A,Lindner K.Sci Technol Weld Joining,2005;10:190 [10]Feng J C,Chen Y C,Liu H J.Mater Sci Technol,2006; 22(1):86 [11]Ren S R,Ma Z Y,Chen L Q,Zhang Y Z.Acta Metall Sin, 2007;43:225 (任淑荣,马宗义,陈礼清,张玉政.金属学报,2007;43:225) [12]Zhang H W,Zhang Z,Chen J T.J Mater Process Technol, 2007;183:62 [13]Zhang Z,Zhang H W.Chin J Mater Res,2006;20:504 (张昭,张洪武.材料研究学报,2006;20:504) [14]Liu H J,Pan Q,Kong Q W,Tang X D,Su L,Li X J,Sun J B,Yang G F.Weld Joining,2007;(2):7 (刘会杰,潘庆,孔庆伟,唐旭东,苏琳,李学军,孙静波,杨国锋.焊接,2007;(2):17) [15]Wang J H,Yao S,Wei L W,Qi X H.Trans Chin Weld Inst,2000;21(4):61 (汪建华,姚舜,魏良武,戚新海.焊接学报,2000;21(4):61) [16]Wang D Y,Feng J C,Wang P F.Trans Chin Weld Inst, 2005;26(3):25 (王大勇,冯吉才,王攀峰.焊接学报,2005;26(3):25) [17]Han X H,Wang X J.Electron Weld Mach,2006;36(11): 48 (韩晓辉,王希靖.电焊机,2006;36(11):48) [18]Zhang Z,Zhang H W.Int J Adv Manuf Technol,DOI: 10.100T/s00170-007-0971-6 [19]Zhao Y H,Lin S B,He Z Q,Wu L.Sci Technol Weld Joining,2006;11:178 [20]Schmidt H,Hattel J.Modell Simul Mater Sci Eng,2005; 13:77 [21]Buffa G,Hua J,Shivpuri R,Fratini L.Mater Sci Eng, 2006;A419:389 [22]Dong P,Lu F,Hong J K,Cao Z.Sci Technol Weld Join- ing,2001;6:281 [23]Bastier A,Maitournam M H,Dang Van K,Roger F.Sci Technol Weld Joining,2006;11:278 [24]Zhang H W,Zhang Z.J Mater Sci Technol,2007;23:73 [25]HKS Co.Ltd.ABAQUS User Manual.Version 6.4,2003 [26]Guerra M,Schmidt C,McClure J C,Murr L E,Nunes A C.Mater Charact,2003;49:95 [27]Zhang H W,Zhang Z.In:Hu P,Reddy J N,eds.,Int Conf on Enhancement and Promotion of Computational Meth- ods in Engineering Science and Mechanics,Changchun: Jinlin University press,2006:52 [28]Zhang Z,Zhang H W.Acta Metall Sin,2006;42:998 (张昭,张洪武.金属学报,2006;42:998) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|