| 高强铝合金焊接接头无析出物区的形成机理 |
| 田志凌;许良红 |
| 钢铁研究总院结构 |
|
| The investigation of the oriented precipitate-free zone in high strength aluminum alloy welds |
| 许良红 Xu Liang-Hong;tian zhiling Tian |
| 钢铁研究总院结构 |
引用本文:
田志凌; 许良红 . 高强铝合金焊接接头无析出物区的形成机理[J]. 金属学报, 2008, 44(1): 91-97 .
,
.
The investigation of the oriented precipitate-free zone in high strength aluminum alloy welds[J]. Acta Metall Sin, 2008, 44(1): 91-97 .
[1]Kramer L S,Blair T P,Blough S D,Pickens J R.Mater Eng Perform,2002;11:645 [2]Carter H B,David H E,Ashok S.Eng Fract Mech,1999; 62(1):1 [3]Fisher J,James J.Adv Mater Process,2002;160(9):43 [4]Devincent S M,Devletian J H,Gedeon S A.Weld J,1988; 67(7):33 [5]Huang C,Kon S.Weld J,2001;80(1):9 [6]Srinivasa R,Madhusudhana R,Prasad R.Mater Sci Eng, 2005;A403:69 [7]Ojo O A,Richards N L,Chaturvedi M C.Scr Mater,2004; 51:141 [8]Bj(?)rneklett B I,Grong (?),Myhr O R,Kluken A O.Sci Technol Weld Joining,1999;4:161 [9]Meyer B C,Doyen H,Emanowski D,Hirsch T,Mayr P. Metall Mater Trans,2000;31A:1454 [10]Wilson A.PhD Thesis,Pennsylvania State University, 2001 [11]Huang C,Kou S.Weld J,2001;80(2):46 [12]Huang C,Kou S.Weld J,2000;79(5):113 [13]Cahn J W.Acta Metall,1961;9:795 [14]Kuo M,Fournelie R A.Acta Metall Mater,1991;39:2835 [15]Barker S W,Purdy G R.Acta Mater,1998;46:511 [16]Nakkalil R,Richards N L,Chaturvedi M C.Acta Metall Mater,1993;41:3381 [17]Ryosnke K,Ikuo O,Kiyohito I.Mater Trans,2003;44: 1768 [18]Tian R Z,Wang Z T.Aluminum and Its Workin9 Hand Book.Changsha:Central and South University Press, 2000:97 (田荣璋,王祝堂.铝合金及其加工手册.长沙:中南大学出版社,2000:97) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|