| 碳钢表面硅烷锌铝涂层的腐蚀电化学行为 |
| 周文娟;许立坤;王佳;李宁;薛丽莉;陈光章 |
| 中国船舶重工集团公司第七二五研究所海洋腐蚀与防护国防科技重点实验室; 青岛 266071 |
|
| study on corrosion electrochemical behavior of silane coating with flaked |
| Zhou Wen-Juan;Likun Xu;Jia Wang;;; |
| 中船重工725所 |
引用本文:
周文娟; 许立坤; 王佳; 李宁; 薛丽莉; 陈光章 . 碳钢表面硅烷锌铝涂层的腐蚀电化学行为[J]. 金属学报, 2007, 43(9): 983-988 .
,
,
,
,
,
.
study on corrosion electrochemical behavior of silane coating with flaked[J]. Acta Metall Sin, 2007, 43(9): 983-988 .
[1]Fourez M,Gheno F,White P E.Trans Inst Met Finish, 1993;71:21 [2]Lonca M.Finishing,1990;14:35 [3]Wynn P.Trans Inst Met Finish,2003;81:16 [4]Bastos A C,Ferreira M G S.Simoes A M.Prog Org Coat, 2005;52:339 [5]Zubielewicz M,Gnot W.Prog Organic Coat,2004;49:358 [6]Le Pen C,Vereecken J.J Appl Electrochem,2005;35: 1303 [7]Ferreira M G S,Duarte R G,Montemo M F,Sim(?)es A M P.Electrochimica Acta,2004;49:2927 [8]Xie D M,Feng H,Ms X C.Corros Sci Prot Technol,2005; 17:237 (谢德明,冯海,马晓春.腐蚀科学与防护技术,2005;17:237) [9]Marchebois H,Savall C,Bernard J,Touzain S.Elec- trochim Acta,2004;49:2945 [10]Zhang J T.Doctoral Dissertation,Zhejiang University, Hangzhou,2005 (张金涛.浙江大学博士学位论文,杭州,2005) [11]Xie D M,Tong S P,Feng H,Zhang J Q.Acta Metall Sin, 2005;41:769 (谢德明,童少平,冯海,张鉴清.金属学报,2005;41:769) [12]Ostanina T N,Rudo V M i,Yaroslavtseva O V,Solov'ev A S,Subbotina O Y,Dokashenko S I.Russ J Electrochem, 2004;40:1019 [13]Wen G N.J Northeast Univ(Nat Sci),1999;20:65 (文光男.东北大学学报(自然科学版),1999;20:65) [14]Marchebois H,Touzain S,Joiret S,Bernard J,Savall C. Prog Org Coat,2002;15:454 [15]Sun Q X,Zhang J Q,Lin C J.Acta Phys Chim Sin,2004; 20:1297 (孙秋霞,张鉴清,林昌健.物理化学学报,2004;20:1297) [16]Xie D M,Hu J M,Tong S P,Wang J M,Zhang J Q.Acta Metall Sin,2004;40:103 (谢德明,胡吉明,童少平,王建明,张鉴清.金属学报,2004;40:103) [17]Senkevich J J.J Mater Sci,2000;35:1359 [18]Liu J G,Gong G P,Yah C W.Electrochim Acta,2005; 50:332. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|