| 焊接残余应力对氢扩散影响的有限元模拟 |
| 蒋文春 巩建鸣 唐建群 陈 虎 涂善东 |
| 南京工业大学机械与动力工程学院; 南京 210009 |
|
| Finite Element Simulation of the Effect of Welding Residual Stress on Hydrogen Diffusion |
| JIANG Wenchun; GONG Jianming; TANG Jianqun; CHEN Hu; TU Shandong |
| College of Mechanical and Power Engineering; Nanjing University of Technology; Nanjing 210009 |
引用本文:
蒋文春; 巩建鸣; 唐建群; 陈虎; 涂善东 . 焊接残余应力对氢扩散影响的有限元模拟[J]. 金属学报, 2006, 42(11): 1221-1226 .
,
,
,
,
,
.
Finite Element Simulation of the Effect of Welding Residual Stress on Hydrogen Diffusion[J]. Acta Metall Sin, 2006, 42(11): 1221-1226 .
[1] Zhang Y R, Dong C F, Li X G, Rui X L, Zhou H R. Acta Metall Sin, 2006; 42: 521 (张颖瑞,董超芳,李晓钢,芮晓龙,周和荣.金属学报,2006; 42:521) [2] Guo H, Li G F, Cai X, Yang W. Acta Metall Sin, 2004; 40: 967 (郭浩,李光福,蔡殉,杨武.金属学报,2004;40:967) [3] Tang J Q, Gong J M, Zhang L J. Corros Sci Prot Technol, 2005; 17: 432 (唐建群,巩建鸣,张礼敬.腐蚀科学与防护技术, 2005;17: 432) [4] Rogante M, Battistella P, Cesari F. Int J Hydrogen Energy, 2006; 31: 597 [5] Tang J Q, Gong J M, Zhang X C, Tu S T. Eng Failure Anal, 2006; 13: 1057 [6] Pandey R K. Eng Failure Anal, 2005; 12: 376 [7] Nyborg R. ASTM STP, 1994: 27 [8] Xue J R. Trans Chin Weld Inst, 1998; 19: 263 (薛继仁.焊接学报,1998;19:263) [9]Zhang T,Yao Y,Chu W Y,Qiao L J.Acta Metall Sin, 2002;38:844 (张涛,姚远,褚武扬,乔利杰.金属学报.2002;38:844) [10] Turnbull A, Ferriss D H. Structural Materials: Properties, Microstructure and Processing, 1996; 206(1): 1 [11] Hughey, Michael P, Cook, Robert F. Appl Phys Lett, 2004; 85: 404 [12] Quan G F. J Chin Soc Corros Prot. 1993; 13: 80 (权高峰.中国腐蚀与防护学报, 1993;13:80 [13] Zhao X W, Su Y J, Gao K W, Qiao L J, Chu W Y, Xu Y. Acta Metall Sin, 2005; 41: 173 (赵显武,宿彦京,高克玮,乔利杰,褚武扬.许颖.金属学报,2005;41:173) [14] Zhang X H, Chen P Y, Tan C Y. Trans Chin Weld Inst, 2002; 23(2): 9 (张显辉,陈佩寅,谭长瑛.焊接学报,2002;23(2):9) [15] Zhang X H, Chen P Y, Tan C Y. Trans Chin Weld Inst, 2000; 21(3): 51 (张显辉,陈佩寅,谭长瑛.焊接学报, 2000;21(3):51) [16] Li Y J, Wang Q. J Mater Proc Technol, 2005; 161(3): 423 [17] Hibbit K. ABAQUS User Manual, 2003 [18] Hirth J P. Metall Trans, 1980; 11A: 861 [19] Teng T L, Lin C C. Int J Pres Vessels Piping, 1998; 75: 857 [20] Li M S, Xie X, Wang L F, Gao L X. Pressure Vessel Technol, 2003; 20(11): 18 (李萌盛,谢霞,王丽芳,高丽霞.压力容器,2003;20(11): 18) [21] Zhao L. Corros Sci Prot Technol, 2005; 17: 349 (赵亮.腐蚀科学与防护技术,2005;17:349) [22] Wang F K. Weldment Structure Engineering Analysis of Pressure Vessel. Beijing: Chemical Industry Press, 1998: 20 (王福宽.压力容器焊接结构工程分析.北京:化学工业出版社, 1998:20) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|