| 控制第二相方向性析出对铁基合金记忆效应的影响 |
| 文玉华 张 伟 李 宁 谢文玲 王杉华 |
| 四川大学材料成型及控制工程系; 成都 610065 |
|
| Influence of Precipitated Direction of the Second Phase on Shape Memory |
| WEN Yuhua; ZHANG Wei ; LI Ning; XIE Wenling; WANG Shanhua |
| College of Manufacturing Science and Engineering; Sichuan University; |
引用本文:
文玉华; 张伟; 李宁; 谢文玲; 王杉华 . 控制第二相方向性析出对铁基合金记忆效应的影响[J]. 金属学报, 2006, 42(11): 1217-1220 .
,
,
,
,
.
Influence of Precipitated Direction of the Second Phase on Shape Memory[J]. Acta Metall Sin, 2006, 42(11): 1217-1220 .
[1] Sato A, Soma K, Mori T. Acta Metall, 1982; 30: 1901 [2] Ostuka H, Yamada H, Maruyama T, Tanahashi H, Matsuda S, Murakaami M. Trans Iron Steel Inst Jpn, 1990; 30: 674 [3] Rong L J, Ping D H, Li Y Y, Shi C X. Scr Metall Mater, 1995; 32: 1905 [4] Kajiwara S. Mater Sci Eng, 1999; A273-275: 67 [5] Wan J F, Huang X, Chen S P, Hsu T Y. Mater Trans, 2002; 43: 920 [6] Liu D Z, Kajiwara S, Kikuchi T, Shinya N. Philos Mag, 2003; 83A: 2875 [7] Wen Y H, Yan M, Li N. Scr Mater, 2004; 50: 441 [8] Wen Y H, Yan M, Li N. Acta Metall Sin, 2004; 40: 72 (文玉华,严密,李宁.金属学报,2004;40:72) [9] Matsumura O, Furusako S, Sumi T, Furukawa T, Otsuka H. Mater Sci Eng, 1999; A272: 459 [10] Wang Z, Cai W, Zhao L C. J Mater Sci Technol, 1998; 14: 182 [11] Kajiwara S, Liu D, Kikuchi T, Shinya N. Scr Mater, 2001; 44: 2809 [12] Pan J S, Tong J M, Tian M B. Elements of Materials Science. Beijing: Tsinghua University Press, 1998: 590 (潘金生,仝健民,田民波.材料科学基础.北京:清华大学出版社,1998:590) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|