| 多晶柱状Cu膜的表面粗化与织构 |
| 杨吉军;马 飞;徐可为 |
| 西安交通大学金属材料强度国家重点实验室 |
|
| SURFACE ROUGHENING AND TEXTURE OF THE POLYCRYSTALLINE COLUMNAR Cu FILMS |
| Jijun Yang; |
| 西安交通大学材料科学与工程学院 |
引用本文:
杨吉军; 马飞; 徐可为 . 多晶柱状Cu膜的表面粗化与织构[J]. 金属学报, 2006, 42(12): 1233-1237 .
,
,
.
SURFACE ROUGHENING AND TEXTURE OF THE POLYCRYSTALLINE COLUMNAR Cu FILMS[J]. Acta Metall Sin, 2006, 42(12): 1233-1237 .
[1] Dumay B, Finot E, Theobald M, Legaie O, Durand J, Baclet P, Goudonnet J P. J Appl Phys, 2002; 92: 6572 [2] Family F, Vicsek T. J Phys, 1985; 18A: L75 [3] Chame A, Reis F D A A. Surf Sci, 2004; 553: 145 [4] Kardar M, Parisi G, Zhang Y C. Phys Rev Lett, 1986; 56: 889 [5] Lai Z W, Sarma S D. Phys Rev Lett, 1991; 66: 2348 [6] Karabacak T, Zhao Y P, Wang G C, Lu T M. Phys Rev, 2001; 64B: 085323 [7] Dalakos G T, Plawsky J P, Persans P D. Phys Rev, 2005; 72B: 205305 [8] Tong W M, Williams R S, Yanase A, Segawa Y, Anderson M S. Phys Rev Lett, 1994; 72: 3374 [9] Knepper R, Messier R. Proc SPIE, 2001; 4467: 87 [10] Xia L F. Duffuaion in Metals. Harbin: Publishing House of Harbin Institute of Technology, 1989: 137 (夏立芳.金属中的扩散.哈尔滨:哈尔滨工业大学出版社,1989: 137) [11] Mullins W W. J Appl Phys, 1957; 28: 333 [12] Herring C. Phys Rev, 1951; 82: 87 [13] Okolo B, Lamparter P, Welzel U, Wagner T, Mittemeijer E J. Thin Solid Films, 2005; 474: 50 [14] Tang W, Xu K W, Wang P, Li X. Acta Metall Sin, 2002; 38: 9 (唐武,徐可为,王平,李弦.金属学报,2002;38:9) [15] Freund L B, Suresh S. Thin Film Materials Stress, Defect Formation and Surface Evolution. Cambridge: Cambridge University Press, 2003: 550 [16] Lita A E, Sanchez J E. Phys Rev, 2000; 61 B: 7692 [17] Siegert M. Phys Rev Lett, 1998; 81: 548 [18] Lukaszew R A, Clarke R. Appl Surf Sci, 2002; 191: 118A |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|