| 脉冲激光合金化形成含非晶相表层的微观组织 |
| 武晓雷 洪友士 |
| 中国科学院力学研究所非线性力学国家重点实验室; 北京 100080 |
|
引用本文:
武晓雷; 洪友士 . 脉冲激光合金化形成含非晶相表层的微观组织[J]. 金属学报, 2000, 36(10): 1041-1044 .
[1] Lin C J, Spaepen H. Appl Phys Lett, 1982; 41: 721 [2] Hirose F, Takagi M, Mori H, Kitoh Y, Imura T. Jpn JAppl Phys, 1992; 31: 3940 [3] Wu X L, Hong Y S. Acta Metall Sin, 2000; 36: 239(武晓雷.洪友士.金属学报.2000;36:239) [4] Follstaedt D M. In: Appleton B R, Celler G K eds., Procof Laser and Electron Beam Interactions with Solids, NewYork: North Holland, 1982: 377 [5] Yatsuya S, Massalski T B. Mater Sci Eng, 1982; 54: 101 [6] Zhang J G, Zhang X M, Lin Y T, Ko T. J Mater Sci,1988; 23: 4357 [7] Sare I R. Scr Metall, 1975; 9: 607 [8] Takayama S. J Mater Sci, 1976; 11: 164 [9] Egami T. Mater Sci Res Bull, 1978; 13: 557 [10] Zhao D Q, Wang W H, Zhuang Y X, Pan M X, Ji Y F,Ma X M, Dong Y D. Sci Chin, 2000; 43A: 307 [11] Swalin R A. Handbook of Thermodynamics Data of Solids.New York: Wiley, 1987: 388 [12] Greer A L. Nature, 1993; 366: 304 |
|