| Ti—B4C反应路径分析 |
| 唐建新 苗赫濯 |
| 北京航空材料研究院; 北京 100095 |
|
引用本文:
唐建新; 苗赫濯 . Ti—B4C反应路径分析[J]. 金属学报, 2000, 36(8): 833-836 .
[1] Ramberg J, Wolf e C, Williams W. J Am Ceram Soc, 1985;C68: 78 [2] Barsoum M W, Houng B. J Am Ceam Soc, 1993; 76(6):1445 [3] Brodkin D, Barsoum M W, Zavaliagos A, Kalidinli S. Ceram Eng Sci Pro, 1994; 15(4): 121 [4] Tang J X, Zuo K F, Hu X Q. J Tsinghua Uniu (Sci Tech),1998; 38(12): 73(唐建新,左开芬,胡晓清.清华大学学报,1998,38(12):73) [5] Tang J X. Ph D Thesis, Tsinghua University, 1999: 72(唐建新.清华大学博士学位论文,1999:72) [6] Broodkin D, Barsoum M W. J Am Ceram Soc, 1996;79(3): 785 [7] Liang Y J, Che Y C. Handbook of Inorganic Thermodynamic Data. Shenyang: Dongbei University Press, 1993:328(梁英教,车荫昌.无机物热力学数据手册.沈阳:东北大学出版社,1993:328)O |
|