| 含Sm的Sb-Mn合金自生复合材料与磁性能 |
| 潘治 孙国雄 |
| 东南大学机械工程系;南京 210018 |
|
引用本文:
潘治; 孙国雄 . 含Sm的Sb-Mn合金自生复合材料与磁性能[J]. 金属学报, 2000, 36(3): 319-324 .
[1] Zhou S Z. Rare-Earth Metal Containing Permanent-MagnetMaterials and Their Applications. Beijing: Metallurgical Industry Press, 1995: 3 (周寿增.稀土永磁材料及其应用.北京,冶金工业出版社,1995:3) [2] Wang Y G. Doctor Thesis, Zhejiang University, 1996 (王寅岗.浙江大学博士学位论文,1996) [3] Pan Y, Sun G X. J Mater Sci, 1998; 33: 763 [4] Pan Y, Sun G X. In: Imura T ed. Proc 4th Special Symposium on Advanced Materials. Nagoya: The CO-OP PrintingBureau of Nagoya University, 1998: 138 [5] Pan Y, Sun G X. Scr Mater, 1999; 41: 803 [6] Pan Y, Sun G X. Acta Metall Sin, 1996; 32: 120 (潘冶,孙国雄.金属学报,1996;32:120) [7] Markandeyulu G, Rama Rao K V S. J Magn Magn Mater,1987; 67: 215 |
|